| 电子探针分析氧化物用的α校正因子的计算及其适用性的讨论 |
| 关若男 |
| 中国科学院金属研究所 |
|
| CALCULATION OF THE α CORRECTION FACTORS FOR ELECTRON MICROPROBE ANALYSIS OF OXIDES AND ITS APPLICABILITY |
| Guan Ruonan Institute of Metal Research; Academia Sinica |
引用本文:
关若男. 电子探针分析氧化物用的α校正因子的计算及其适用性的讨论[J]. 金属学报, 1980, 16(3): 341-348.
.
CALCULATION OF THE α CORRECTION FACTORS FOR ELECTRON MICROPROBE ANALYSIS OF OXIDES AND ITS APPLICABILITY[J]. Acta Metall Sin, 1980, 16(3): 341-348.
[1] Ziebold, T. O. and Ogilvei, R. E., Anal. Chem 36 (1964) , 322. [2] Ingersoll, R. M., Taylor, J. E. and Derouin, D. H., Advances in X-Ray Analysis, vol. 9, Plenum, New York, 1965, p. 273. [3] Albee, A. L. and Ray, L., Analy. Chem., 42 (1970) , 1408. [4] Bence, A. C. and Albee, A. L., J. Geol., 76 (1968) , 382. [5] 金属研究所,金属材料研究,1976,№ 7, p. 452. [6] Toshio Shiraiwa and Nobukatsu Fujine, Jap. J. Appl. Phys., 9 (1970) , 976. [7] Heinrich, K. F. J., The Electron Microprobe, ed. by T.D. McKinley et al., Wiley, New York, 1966, p, 296. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|