| 用Marx法精确测量内耗和弹性模量时的计算公式 |
| 孙宗琦 |
| 中国科学院金属研究所 |
|
| FORMULAE FOR MEASURING INTERNAL FRICTION AND MODULUS BY MARX METHOD |
| Sun Zongqi (Institute of Metal Research; Academia Sinica; Shenyang) |
引用本文:
孙宗琦. 用Marx法精确测量内耗和弹性模量时的计算公式[J]. 金属学报, 1982, 18(6): 726-734.
.
FORMULAE FOR MEASURING INTERNAL FRICTION AND MODULUS BY MARX METHOD[J]. Acta Metall Sin, 1982, 18(6): 726-734.
1 孙宗琦,金属学报,18(1982) ,293. 2 Marx, J., Rev. Sci. Instrum., 22(1951) , 503. 3 Beshers, D. N., Techniques of Metals Research, Vol. Ⅶ, Part 2, Ed. Bunshah, R. F., Wiley, New York, 1976, p. 618. 4 Cady, W. G., Piezoelectricity, McGraw-Hill, 1946, p. 88. 5 Minorsky, N., Nonlinear Oscillation, Van Nostrand, New York, 1969, p. 375. 6 Robinson, W. H.; Edgar, A., IEEE Trans. Sonics Ultrason., SU-21(1974) , 98. 7 Robinson, W. H.; Carpenter, S. H.; Tallon, J. L., J. Appl. Phys., 45(1974) , 1975. 8 Robinson, W. H., Philos. Mag., 25(1972) , 355. 9 Huber, R. J.; Baker, G. S.; Girrs, P., J. Appl. Phys., 32(1961) , 2488. 10 Baker, G. S.; Carpenter, S. H., Rev. Sci. Instrum., 36(1965) , 29. 11 Devine, S. D.; Robinson, W. H., J. Appl. Phys, 48(1977) , 1437. 12 Simpson, M.; Finlayson, T. R.; Smith, T. F., J. Phys. D11(1978) , 453. 13 Nowick, A. S.; Berry, B. S., Anelastic Relaxation in Crystalline Solids, Academic Press, 1972, p. 431. 14 Schwarz, R. B., Rev. Sci. Instrum., 48(1977) , 111. 15 Tatento, H.; Tanignchi, H., Jpn. J. Appl. Phys., 19(1980) , 175. 16 Wuttig, M.; Suzuki, T., Acta Metall., 27(1979) , 755. 17 Wuttig, M.; Suzuki, T., Scr. Metall., 14(1980) , 229. 18 Ritchie, I. G.; Atrens, A.; Blair, D. G., Internal Friction and Ultrasonic Attenuation in Solids, Ed. Hasiguti, R. R., Uni. Tokyo Press, 1977, p. 637. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|