| Fe-Al合金相及相变的价电子结构分析 |
| 左秀忠 |
| 东北工学院 |
|
| STRUCTURAL ANALYSIS OF VALENCE ELECTRON IN Fe-Al ALLOY PHASE AND ITS TRANSFORMATION |
| Zuo Xiuzhong (North East Institute of Technology; Shenyang) |
引用本文:
左秀忠. Fe-Al合金相及相变的价电子结构分析[J]. 金属学报, 1982, 18(6): 735-745.
.
STRUCTURAL ANALYSIS OF VALENCE ELECTRON IN Fe-Al ALLOY PHASE AND ITS TRANSFORMATION[J]. Acta Metall Sin, 1982, 18(6): 735-745.
1 余瑞璜,科学通报,23(1978) ,217. 2 余瑞璜,科学通报,26(1981) .206. 3 余瑞璜,吉林大学自然科学学报,(1979) ,№4,54. 4 Pearson, W. B., Structure Reports, 1958 Vol. 22, Int. Union Cryst., Utrecht, 1968, p. 14. 5 Berkowitz, A. E.; Kneller, E., Magnetism and Metallurgy, Vol.2, Academic Press, 1969, p. 561. 6 Bozorth, R. M., Ferromagnetism, Van Nostrand, Canada, 1955, p. 215.k |
|