| 热轧组织和织构对3%和4%Si-Fe合金冷加工性能的影响 |
| 吕其春;张文润;帅仁杰;李俊义 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| EFFECT OF STRUCTURE AND TEXTURE ON COLD WORKABILITY OF 3%-AND 4%Si-Fe ALLOYS |
| LU Qichun; ZHANG Wenrun; SHUAI Renjie; LI Junyi (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
引用本文:
吕其春;张文润;帅仁杰;李俊义. 热轧组织和织构对3%和4%Si-Fe合金冷加工性能的影响[J]. 金属学报, 1983, 19(6): 36-44.
,
,
,
.
EFFECT OF STRUCTURE AND TEXTURE ON COLD WORKABILITY OF 3%-AND 4%Si-Fe ALLOYS[J]. Acta Metall Sin, 1983, 19(6): 36-44.
1 Arai, K.I. Tsuya, N.; Ohmori, K.; Shimanaka, H.; Miyazaki, T., J. Magn Magn Mater, 15-18 (1980) , 1425. 2 Narita, K.; Teshima, N.; Agano, T.; Funahashi, H., IEEE Trans. Magn., MAG-16 (1980) , 517. 3 Fiedler, H.C., J. Iron Steer Inst., 205 (1967) , 158. 4 Burr, D.J.; Butt, R.J.; Wakeman, D.W., J. Iron Steer Inst., 203 (1965) , 500. 5 #12 6 #12 7 Clark, C.A.; Mason, J.J., Patent Specification, №982 101, 1965. (England). 8 Clark, C.A.; Mason, J.J.; Mee, P.B., Proc. IEE, 113 (1966) , №2, 345. 9 吕其春;张文润;李军;李俊义,冶金因素对高硅硅钢冷加工性能的影响,待发表. 10 Lu Qichun; Shuai Renjie; Zhou Xiuyuan, Proc. of the 6th Int. Conf. on Textures of Materials, Vol. 2, 1981, Tokyo, Ed. Nagashima, S.I., Publ. Iron and Steel Inst. Jpn, p.958-966. |
|