| Nb-V微合金钢中Nb与V析出相的精细结构 |
| 徐温崇;孙福玉 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| THE FINE STRUCTURE OF Nb AND V PRECIPITATES IN Nb-V STEEL |
| XU Wenchong; SUN Fuyu (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
引用本文:
徐温崇;孙福玉. Nb-V微合金钢中Nb与V析出相的精细结构[J]. 金属学报, 1983, 19(6): 29-118.
,
.
THE FINE STRUCTURE OF Nb AND V PRECIPITATES IN Nb-V STEEL[J]. Acta Metall Sin, 1983, 19(6): 29-118.
1 Baker, R. G.; Nutting, J., Iron Steel Inst., London, Spec. Rep., (1959) , №. 64, 1. 2 Chaturvedi, M. C,; Honeycombe, R.W.K.; Warrington, D.H., J. Iron Steel Inst., 206 (1968) , 1236. 3 Billingham, J.; Bell, P. S.; Lewis M.H., Acta Crystallogr., A28 (1972) , 602. 4 Froidevaux, C.; Rossier, D., J. Phys. Chem. Solids, 28 (1967) , 1197. 5 Prnka, T., Second Internal Conference on the Strength of Metals and Alloys, Vol.2, ASM 1970, p.590. 6 Bourgeot, J.,私人通讯. 7 成田贵一;小山伸二;铁鋼,52 (1966) ,788. 8 Irvine, K.J.; Pickering, F. B.; Gladman, T., J. Iron Steel Inst., 205 (1967) , 161. 9 待发表. 10 Duwez, P.; Odell, F., J. Electrochem. Soc., 97 (1950) , 299. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|