| W-Ni-Fe两相合金的形变强化与组织结构 |
| 朱桂森;刘铭成;甄振先 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| WORK STRENGTHENING OF BIPHASE W-Ni-Fe ALLOYS AND THEIR MICROSTRUCTURE |
| ZHU Guisen; LIU Mingcheng; ZHEN Zhenxian (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry Beijing) |
引用本文:
朱桂森;刘铭成;甄振先. W-Ni-Fe两相合金的形变强化与组织结构[J]. 金属学报, 1983, 19(6): 45-120.
,
,
.
WORK STRENGTHENING OF BIPHASE W-Ni-Fe ALLOYS AND THEIR MICROSTRUCTURE[J]. Acta Metall Sin, 1983, 19(6): 45-120.
1 Krock, R.H.; Shepard, L.A., Trans. Metall. Soc. AIME, 227 (1963) , 1127. 2 #12 3 Ekbom, L., Scand. J. Metall., 5 (1976) , 179. 4 Northcutt, W.G., Jr., Y/DA-6666, 1976, p. 13. 5 朱桂森;刘铭成;林忠杰;俞淑延,金属学报,17(1981) ,39. 6 Ariel, E.; Barta, J.; Brandon, D., Powder Metall, Int., 5 (1973) , 126 7 #12 |
|