金属学报  1985, Vol. 21 Issue (1): 134-138    
  论文 本期目录 | 过刊浏览 |
用γ-γ角关联方法测量Ni的超精细场
倪新伯;刘根宝;杨锦晴;蒋大真;徐金龙
中国科学院上海原子核研究所;中国科学院上海原子核研究所;中国科学院上海原子核研究所;中国科学院上海原子核研究所;中国科学院上海原子核研究所
MEASUREMENT OF HYPERFINE FIELD IN Ni BY MEANS OF γ-γ AUGULAR CORRELATION METHOD
NI Xinbo;LIU Kenpao;YANG Jinqing;JIANG Dazhen;XU Jinlong Shanghai Institute of Nuclear Research;Academia Sinica
引用本文:

倪新伯;刘根宝;杨锦晴;蒋大真;徐金龙. 用γ-γ角关联方法测量Ni的超精细场[J]. 金属学报, 1985, 21(1): 134-138.
, , , , . MEASUREMENT OF HYPERFINE FIELD IN Ni BY MEANS OF γ-γ AUGULAR CORRELATION METHOD[J]. Acta Metall Sin, 1985, 21(1): 134-138.

全文: PDF(378 KB)  
摘要: 本文利用时间微分扰动角关联(TDPAC)方法,以~(111)Cd为探测原子核,测量了高纯Ni样品中作用于~(111)Cd溶质离子的超精细磁场强度.
Abstract:The time differential perturbed angular correlation(TDPAC)method was em-ployed for the measurement of the hyperfine magnetic field of ~(111)Cd solute ions inhigh purity Ni.The experimental results were analysed and discussed.This trialprovides leads for further research on the hyperfine field in the ferromagnetic metalsand rare-earth elements.
收稿日期: 1985-01-18     
1 Grace,M.A.;Johnson,C.E.;Kurti,N.;Scurlock,R.G.;Taylor,R.T.,Proc.of the Conf.on the Physical Basses of Temperature,Paris,1955,(Unpublished).
2 Khutsishvili,G.R.,Soviet Phys.-JETP,2(1956) ,894.
3 Freeman,A.J.;Watson,R.E.,Magnetism,Eds.Rado,G.T.;Suhl,H.,Academic Press,New York,1965,Vol.IIA,p.168.
4 #12
5 Karlsson,E.;Matthias,E.;Siegbahn,K.,Perturbed Angular Correlations,North-Holland,Amsterdam,1964.
6 扰动角关联组,核技术,1(1979) ,32.