| 关于固溶体晶格常数的预测 |
| 宁远涛;徐桦 |
| 冶金工业部贵金属研究所;中国科学院上海冶金研究所 |
|
| AN APPROACH TO PREDICTING LATTICE PARAMETERS OF CERTAIN SOLID SOLUTION |
| NING Yuantao Institute of Precious Metals;Kunming;XU Hua Shanghai Institute of Metallurgy;Academia Sinica |
引用本文:
宁远涛;徐桦. 关于固溶体晶格常数的预测[J]. 金属学报, 1985, 21(1): 139-144.
,
.
AN APPROACH TO PREDICTING LATTICE PARAMETERS OF CERTAIN SOLID SOLUTION[J]. Acta Metall Sin, 1985, 21(1): 139-144.
1 Moreen,H.A.,Taggart,R.;Polonis,D.D.,Metall.Trans.,2(1971) ,265. 2 Jones,H.,Scr.Metall.,17(1983) ,97. 3 Miedema,A.R.,J.Less-Common Met.,32(1973) ,117. 4 Miedema,A.R.,ibid.,46(1976) 71. 5 Pearson,W.B.;A Handbook of Lattice Spacings and Structures of Metals and Alloys,Pergamon Press,New York,1958,p.304,331. 379,610. 6 宁远涛;郑云,金属学报,19(1983) ,B225. 7 周新铭;靳嘉禄;宁远涛;赵钟民,金属学报,18(1982) ,534. |
|