| 用γ-γ角关联方法测量Ni的超精细场 |
| 倪新伯;刘根宝;杨锦晴;蒋大真;徐金龙 |
| 中国科学院上海原子核研究所;中国科学院上海原子核研究所;中国科学院上海原子核研究所;中国科学院上海原子核研究所;中国科学院上海原子核研究所 |
|
| MEASUREMENT OF HYPERFINE FIELD IN Ni BY MEANS OF γ-γ AUGULAR CORRELATION METHOD |
| NI Xinbo;LIU Kenpao;YANG Jinqing;JIANG Dazhen;XU Jinlong Shanghai Institute of Nuclear Research;Academia Sinica |
引用本文:
倪新伯;刘根宝;杨锦晴;蒋大真;徐金龙. 用γ-γ角关联方法测量Ni的超精细场[J]. 金属学报, 1985, 21(1): 134-138.
,
,
,
,
.
MEASUREMENT OF HYPERFINE FIELD IN Ni BY MEANS OF γ-γ AUGULAR CORRELATION METHOD[J]. Acta Metall Sin, 1985, 21(1): 134-138.
1 Grace,M.A.;Johnson,C.E.;Kurti,N.;Scurlock,R.G.;Taylor,R.T.,Proc.of the Conf.on the Physical Basses of Temperature,Paris,1955,(Unpublished). 2 Khutsishvili,G.R.,Soviet Phys.-JETP,2(1956) ,894. 3 Freeman,A.J.;Watson,R.E.,Magnetism,Eds.Rado,G.T.;Suhl,H.,Academic Press,New York,1965,Vol.IIA,p.168. 4 #12 5 Karlsson,E.;Matthias,E.;Siegbahn,K.,Perturbed Angular Correlations,North-Holland,Amsterdam,1964. 6 扰动角关联组,核技术,1(1979) ,32. |
|