| 环境介质对GH36合金低循环疲劳寿命的影响 |
| 王栓柱;王兴国;崔遂玲 |
| 西安航空发动机厂;西安航空发动机厂;西安航空发动机厂 |
|
| LCF LIFE OF SUPERALLOY GH36 IN VARIOUS ENVIRONMENTS |
| WANG Shuanzhu WANG Xingguo CUI Suiling (Xi'an Aero-engine Factory) |
引用本文:
王栓柱;王兴国;崔遂玲. 环境介质对GH36合金低循环疲劳寿命的影响[J]. 金属学报, 1987, 23(1): 76-81.
,
,
.
LCF LIFE OF SUPERALLOY GH36 IN VARIOUS ENVIRONMENTS[J]. Acta Metall Sin, 1987, 23(1): 76-81.