| 盐对GH37镍基合金蠕变性能的影响 |
| 曹名洲;秦荣士;赵吉祥 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| EFFECT OF SALTS ON CREEP BEHAVIOUR OF Ni-BASE ALLOY GH37 |
| CAO Mingzhou QIN Rongshi ZHAO Jixiang (Institute of Metal Research.Academia Sinica.Shenyang) |
引用本文:
曹名洲;秦荣士;赵吉祥. 盐对GH37镍基合金蠕变性能的影响[J]. 金属学报, 1987, 23(1): 70-75.
,
,
.
EFFECT OF SALTS ON CREEP BEHAVIOUR OF Ni-BASE ALLOY GH37[J]. Acta Metall Sin, 1987, 23(1): 70-75.
1 Segueira C A,Hocking M G.Corrosion,1981;37:392 2 郭建亭.能源材料通讯,1983;(1) :34 3 姜晓霞.冶金标准化,1983;(2) :34 |
|