| 理论计算和实验测定相结合构筑熔盐相图 |
| 乔芝郁;段淑贞;桂玮珍;孙民生 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| CONSTRUCTION OF MOLTEN SALT PHASE DIAGRAMS BY COMBINATION OF CALCULATION WITH MEASUREMENT |
| by QIAO Zhiyu; DUAN Shuzhen; GUI Weizhen; SUN Minsheng (Beijing University of Iron and Steel Technology) (Manuscript received 31 March; 1986; revised manuscript 24 November; 1986) |
引用本文:
乔芝郁;段淑贞;桂玮珍;孙民生. 理论计算和实验测定相结合构筑熔盐相图[J]. 金属学报, 1987, 23(4): 357-362.
,
,
,
.
CONSTRUCTION OF MOLTEN SALT PHASE DIAGRAMS BY COMBINATION OF CALCULATION WITH MEASUREMENT[J]. Acta Metall Sin, 1987, 23(4): 357-362.
1 CALPHAD Jounral, Pergamon, 1977-1987 2 Pelton A D. AIME Conference Proceedings, Toronto Canada, 1986或:稀有金属 (国际),1987; 6 (1) : 54; (2) : 117 3 Hillerr M.在北京钢铁学院的讲稿,北京1980 4 乔芝郁,Hillert M.北京钢铁学院学报,1981;(1) :109,1981;(3) :77 5 乔芝郁, Hillert M. CALPHAD J, 1985; 9(2) :143 6 Eriksson G. Acta Chem Scand, 1971; 25:2651 7 Eriksson G. Chem Scr, 1975; 8:100 8 Besmann T M. Oak Ridge National Lab Oak Ridge Report ORNLTM, 1977:5575 9 郭祝崑等,1984年全国第三届相图学术会议论文汇编,第一册,昆明,1984 10 Pelton D,乔芝郁,私人通讯 11 乔芝郁.见:段淑贞,乔芝郁主编,熔盐物理化学和电化学,北京:冶金工业出版社,(待发表) 12 李瑞青,乔芝郁,段淑贞,周国治,北京钢铁学院学报,1987;(3) 13 Hillert M. CALPHAD J, 1980; 4(1) :1 14 乔芝郁,莫雯静,武世民,朱元凯,稀有金属(国际版),1983;2(2) :163 15 周国治,CALPHAD J,1987;11(2) 183 16 陈征宇,周国治.1986年全国第四届相图学术会议论文汇编,长沙,1986 17 Qiao Zhiyu (乔芝郁). Sangster J, Pelton A D. CALPHAD J, 1987; 11(4) 18 李瑞青,乔芝郁,段淑贞,周国治.1986年全国第四届相图学术会议论文汇编,长沙,1986 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|