Please wait a minute...
金属学报  1987, Vol. 23 Issue (4): 357-362    
  论文 本期目录 | 过刊浏览 |
理论计算和实验测定相结合构筑熔盐相图
乔芝郁;段淑贞;桂玮珍;孙民生
北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院
CONSTRUCTION OF MOLTEN SALT PHASE DIAGRAMS BY COMBINATION OF CALCULATION WITH MEASUREMENT
by QIAO Zhiyu; DUAN Shuzhen; GUI Weizhen; SUN Minsheng (Beijing University of Iron and Steel Technology) (Manuscript received 31 March; 1986; revised manuscript 24 November; 1986)
引用本文:

乔芝郁;段淑贞;桂玮珍;孙民生. 理论计算和实验测定相结合构筑熔盐相图[J]. 金属学报, 1987, 23(4): 357-362.
, , , . CONSTRUCTION OF MOLTEN SALT PHASE DIAGRAMS BY COMBINATION OF CALCULATION WITH MEASUREMENT[J]. Acta Metall Sin, 1987, 23(4): 357-362.

全文: PDF(475 KB)  
摘要: 本文阐述了相图计算的基本原理和确定体系中各相的全摩尔和偏摩尔过剩自由能的方法,特别是由二元系性质预示三元系性质的几何模型.在指出相图计算的意义和局限性的同时,阐明了理论计算和实验测定相结合是构筑熔盐相图的最佳方法及该方法的主要步骤.
Abstract:The principle and mathods of calculation of phase diagram, especially the geometric models for determination of excess molar Gibbs energy and excess partial molar Gibbs energy in all phases have been reviewed. Considering the significance and the limitation of calculation of phase diagram, it is pointed out that the combination of calculation with measurement is the best method for construction of molten salt phase diagrams. The procedure of this method have also been described.
收稿日期: 1987-04-18     
基金资助:国家自然科学基金资助课题
1 CALPHAD Jounral, Pergamon, 1977-1987
2 Pelton A D. AIME Conference Proceedings, Toronto Canada, 1986或:稀有金属 (国际),1987; 6 (1) : 54; (2) : 117
3 Hillerr M.在北京钢铁学院的讲稿,北京1980
4 乔芝郁,Hillert M.北京钢铁学院学报,1981;(1) :109,1981;(3) :77
5 乔芝郁, Hillert M. CALPHAD J, 1985; 9(2) :143
6 Eriksson G. Acta Chem Scand, 1971; 25:2651
7 Eriksson G. Chem Scr, 1975; 8:100
8 Besmann T M. Oak Ridge National Lab Oak Ridge Report ORNLTM, 1977:5575
9 郭祝崑等,1984年全国第三届相图学术会议论文汇编,第一册,昆明,1984
10 Pelton D,乔芝郁,私人通讯
11 乔芝郁.见:段淑贞,乔芝郁主编,熔盐物理化学和电化学,北京:冶金工业出版社,(待发表)
12 李瑞青,乔芝郁,段淑贞,周国治,北京钢铁学院学报,1987;(3)
13 Hillert M. CALPHAD J, 1980; 4(1) :1
14 乔芝郁,莫雯静,武世民,朱元凯,稀有金属(国际版),1983;2(2) :163
15 周国治,CALPHAD J,1987;11(2) 183
16 陈征宇,周国治.1986年全国第四届相图学术会议论文汇编,长沙,1986
17 Qiao Zhiyu (乔芝郁). Sangster J, Pelton A D. CALPHAD J, 1987; 11(4)
18 李瑞青,乔芝郁,段淑贞,周国治.1986年全国第四届相图学术会议论文汇编,长沙,1986