金属学报  1987, Vol. 23 Issue (4): 382-384    
  论文 本期目录 | 过刊浏览 |
NaF-CaCl_2-LiCl系熔盐相图的研究
阎立诚;杨金秀;朱鹦鹦
上海科技大学;上海科技大学;上海科技大学
PHASE DIAGRAM OF NaF-CaCl_2 -LiCl SYSTEM
by YAN Licheng; YANG Jinxiu; ZHU Yingying (Shanghai University of Science and Technology) (Manuscript received 6 January; 1986; revised manuscript 21 July; 1986)
引用本文:

阎立诚;杨金秀;朱鹦鹦. NaF-CaCl_2-LiCl系熔盐相图的研究[J]. 金属学报, 1987, 23(4): 382-384.
, , . PHASE DIAGRAM OF NaF-CaCl_2 -LiCl SYSTEM[J]. Acta Metall Sin, 1987, 23(4): 382-384.

全文: PDF(224 KB)  
摘要: <正> 用目测变温和X射线相分析,研究了NaF-CaCl_2-LiCl系熔盐相图.在此基础上估算了熔盐的正负偏差,并对其结果进行了讨论. 熔盐相图,除在研究各种熔盐性质及相互作用方面有重大意义外,还有许多实际应用价值.
Abstract:The phase diagram of NaF-CaCl_2-LiCl system was studied by X-ray phase analysis. It was found that the NaF forms negative deviation molten salt solution with CaG_2-LiCl system. This result was discussed based on some conclusion obtained from the Monte-Carlo simulation of molten salt mixture.
收稿日期: 1987-04-18     
1 阎立诚,朱鸚鹦,陈念贻.高等学校化学学报,1984;6(5) :755
2 Grube G, Rucel W.JCP Reference Data, 1975; 4(4) : 959
3 #12
4 #12
5 #12
6 #12
7 陈念贻,张桂成,金属学报,1961;7:11
No related articles found!