| 氢对纯铁屈服行为的影响 |
| 隗学礼;J.Felefli;W.Dahl;K.W.Lange |
| 中国科学院金属研究所;西德Aachen工业大学;西德Aachen工业大学;西德Aachen工业大学 |
|
| INFLUENCE OF HYDROGEN ON YIELDING BEHAVIOUR OF IRON |
| by WEI Xueli(Institute of Metal Research; Academia Sinica Shenyang);FELEFLI; J.; DAHL; W.; LANGE; K.W. (Technical University Aachen; West Germany)(Manuscript received 1 Appril; 1986; revised manuscript 11 September; 1986) |
引用本文:
隗学礼;J.Felefli;W.Dahl;K.W.Lange. 氢对纯铁屈服行为的影响[J]. 金属学报, 1987, 23(5): 437-440.
,
,
,
.
INFLUENCE OF HYDROGEN ON YIELDING BEHAVIOUR OF IRON[J]. Acta Metall Sin, 1987, 23(5): 437-440.
1 Bernstein I M. Sci Metall, 1974; 8: 343 2 Kimura H, Matsui H, Kimura T. In. Suzuki T ed., Proc 2nd JIM Int Symp, Hydrogen in Metals, Japan: JIM, 1979: 533 3 Oriani R A, Josephic P H. Metall Trans, 1980; 11A: 1809 4 Felefli Y, Dahl W, Lange K W. In: 3rd Int Congress on Hydrogen and Materials, Vol. 1, Paris, 1982: 539 5 Cracknell A, Fetch N J. Acta Metall, 1955; 3: 200 6 Dadian M, Talbot-Besnards. C R Hebd Seances Acad Sci, 1963; 256: 5348 7 Vaughan H G, De Morton M E. Acta Metall, 1956; 4: 224 8 Troiano A R, Trans ASM, 1960; 52: 55 9 Rendulic K D. In: Appoications of Field Ion Microscopy in Physica Metallurgy and Corrosion, Georgia Inst Tech Atlanta, 1969: 413 10 Au J J, Birnbaum H K. Acta Metall, 1978; 26: 1105c |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|