| 氢对Ti-15Mo合金形变行为的影响 |
| 杨柯;万晓景;曹名洲 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| EFFECT OF HYDROGEN ON THE DEFORMATION BEHAVIORS FOR Ti-15Mo ALLOY |
| by YANG Ke; WAN Xiaojing; CAO Mingzhou(Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 13 December; 1986) |
引用本文:
杨柯;万晓景;曹名洲. 氢对Ti-15Mo合金形变行为的影响[J]. 金属学报, 1987, 23(5): 441-443.
,
,
.
EFFECT OF HYDROGEN ON THE DEFORMATION BEHAVIORS FOR Ti-15Mo ALLOY[J]. Acta Metall Sin, 1987, 23(5): 441-443.
1 Kimura H, Matsui H, Kimura A, Kimura T, Oguri K. In: Bernstein I M, Thompson A W eds., Hydrogen Effects in Metals, New York: AIME, 1981: 191 2 Kimura H, Matsui H, Moriya S. Mater Sci Eng, 1979; 40: 217 3 Beachem C D. Metall Trans, 1972; 3: 437 4 褚武扬,肖纪美,李世琼。金属学报,1981;17:10 5 褚武扬,肖纪美,李世琼.朱淑彦.金属学报,1982;18:47 6 杨柯.氢在Ti-5Mo合金中行为的研究, 金属研究所硕士论文,1985 7 Johnston W G. Gilman J J.J Appl Phys, 1959; 30: 129 8 Li J C M. Can J Phys, 1967; 45: 493 9 Agrawal S P, Sargent G A, Conrad H. Metall Trans, 1973; 4: 2613 10 Troiano A R. Trans ASM, 1960; 52: 54 11 万晓景,杨柯,曹名洲.金属学报,1986;22:A189 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|