| γ强化镍基合金蠕变摩擦应力的测定 |
| 阳志安;肖耀天;师昌绪 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| CREEP FRICTION STRESS OF γ' STRENGTHENED Ni-BASE SUPERALLOYS |
| by YANG Zhi'an; XIAO Yaotian; SHI Changxu(C. H. Shih) (Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 10 Octorber; 1985; revised manuscript 22 Appril; 1986) |
引用本文:
阳志安;肖耀天;师昌绪. γ强化镍基合金蠕变摩擦应力的测定[J]. 金属学报, 1987, 23(5): 434-436.
,
,
.
CREEP FRICTION STRESS OF γ' STRENGTHENED Ni-BASE SUPERALLOYS[J]. Acta Metall Sin, 1987, 23(5): 434-436.
1 Lund R W, Nix W D. Acta Metall, 1976; 24: 469 2 Ajaja O. Howson T E, Purushothaman S, Tien J K. Mater Sci. Eng, 1980; 44: 165 3 阳志安,肖耀天,师昌绪,金属学报.1983;19:A300 4 Lagneborg R. J Mater Sci, 1968; 3: 596 5 Threadgill P L, Wilshire B. Creep Strength in Steel and High-Temperature Alloys, ISI, Sheffield, 1972, London: Metals Society 1974 6 Williams K R, Wilshire B. Met Sci J, 1973: 7: 176 7 Williams K R, Wilshire B. Mater Sci Eng, 1977; 28: 289 8 McLean M. Scr Metall, 1979; 13: 339 9 McLean M. Proc R Soc London, 1980; A371: 279 10 Friedel J. Dislocations, Oxford: Pergamon, 1964: 239 11 Yang Z A, Xiao Y T, Shih C H. High Temperature Technique, 1987; (2) 12 阳志安.博士论文,中国科学院金属研究所,1985 13 Yang Z A, Xiao Y T, ShihCH. In,Proc Int Conf on Creep' 86, Tokyo, 1986 14 Stevens R A, Flewitt P E J. Acta Met all, 1981; 29: 867 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|