| 镍基高温合金中M_(23)C_6相的选择性阳极浸蚀过程的研究 |
| 张建中;王景韫 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| SELECTIVE ANODIC DISSOLUTION PROCESS OF M23C6 IN A Ni-BASE SUPERALLOY |
| by ZHANG Jianzhong; WANG Jingyun (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 23 July; 1986.; revised manuscript 13 February; 1987) |
引用本文:
张建中;王景韫. 镍基高温合金中M_(23)C_6相的选择性阳极浸蚀过程的研究[J]. 金属学报, 1987, 23(6): 568-574.
,
.
SELECTIVE ANODIC DISSOLUTION PROCESS OF M23C6 IN A Ni-BASE SUPERALLOY[J]. Acta Metall Sin, 1987, 23(6): 568-574.
1#12 2 #12 3 #12 4 #12 5 马翔.分析化学,1984;12(6) 496 6 傅岩松.浸蚀定量法在耐热钢相分析中的应用及其理论基础探讨,金属研究所硕士学位论文,1985 |
|