Please wait a minute...
金属学报  1987, Vol. 23 Issue (6): 568-574    
  论文 本期目录 | 过刊浏览 |
镍基高温合金中M_(23)C_6相的选择性阳极浸蚀过程的研究
张建中;王景韫
中国科学院金属研究所;中国科学院金属研究所
SELECTIVE ANODIC DISSOLUTION PROCESS OF M23C6 IN A Ni-BASE SUPERALLOY
by ZHANG Jianzhong; WANG Jingyun (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 23 July; 1986.; revised manuscript 13 February; 1987)
引用本文:

张建中;王景韫. 镍基高温合金中M_(23)C_6相的选择性阳极浸蚀过程的研究[J]. 金属学报, 1987, 23(6): 568-574.
, . SELECTIVE ANODIC DISSOLUTION PROCESS OF M23C6 IN A Ni-BASE SUPERALLOY[J]. Acta Metall Sin, 1987, 23(6): 568-574.

全文: PDF(451 KB)  
摘要: 在12%(NH_4)_2SO_4水溶液(调pH=9)中,电位在200—800mV(SCE)范围内实现了M_(17)G镍基高温合金中M_(23)C_6相的选择性阳极浸蚀。用线性扫描电位法和恒电位阶跃法研究了浸蚀过程,建立了电化学极化控制下细小、弥散相的选择性阳极浸蚀过程模型。
Abstract:The particles of M_(23)C_6 precipitate in Ni-base superalloy M17G were selectively dissolved in an aqueous solution of 12%(NH_4)_2SO_4 (pH-value was adjusted to 9) in the potential range of +200 to +800 mV (S. C. E.). The anodie dissolution process has been investigated in terms of potential-sweep and potential-step polarization techniques. For the finely dispersive phase in the alloy, a new model has been developed to describe the selective anodic dissolution process, which is eontrolled by electrochemical polarization.