| 含铌铁水-铌渣的平衡和渣中α_(Nb_2O_5)的测定 |
| 陈伟庆;周荣章;林宗彩 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| THE INVESTIGATION OF EQUILIBRIUM BETWEEN SLAG AND HOT METAL CONTAINING Nb AND MEASUREMENT OF αNb_2O_5 IN THE SLAG |
| by CHEN Weiqing; ZHOU Rongzhang; LIN Zongcai (Beijing University of Iron and Steel Technology) (Manuscript received 6 June; 1986; revised manuscript 6 October; 1986) |
引用本文:
陈伟庆;周荣章;林宗彩. 含铌铁水-铌渣的平衡和渣中α_(Nb_2O_5)的测定[J]. 金属学报, 1987, 23(6): 560-567.
,
,
.
THE INVESTIGATION OF EQUILIBRIUM BETWEEN SLAG AND HOT METAL CONTAINING Nb AND MEASUREMENT OF αNb_2O_5 IN THE SLAG[J]. Acta Metall Sin, 1987, 23(6): 560-567.
| 1 福沢章.钢铁,1984;19(8) :56
2 陈伟庆,周荣章,林宗彩.钢铁,1987;22(5) :7
3 Schmalzried H. Ber Bunsenges Phys Chem, 1962; 66: 572
4 Elliott J F. Thermochemistry for Steeimaking, Vol. Ⅱ, Mass: Addison-Wesley, 1963
5 Janke D, Fischer W A. Arch Eisenhuettenwes, 1975; 46: 755
6 郭上型,唐仲和,张永定.全国第五届冶金物化年会论文集(上册),1984:157
7 罗晨,苏良赫.包钢含铌炼钢渣工业岩石学研究,武汉地质学院北京研究生部研究生论文,1983
8 Sigworth G K, Elliott J F. Met Sci, 1974; 8: 298
9 魏寿昆,张圣弼,佟亭,谭赞麟,钢铁.1984;19(7) :1
10 Schenck H, Steinmetz E. Wirkungsparameter Von Beglcitelementen flussiger Eisenloesungen und ihre gegenseitigen Beziehungen, Duesseldorf: Stahleisen-Sonderberichte, 1968: 39
11 日本铁钢学会.铁钢便霓,Ⅰ基礎,表1,3,第3版,东京:丸善,1981:22
12 张圣弼,佟亭,王济舫,魏寿昆.金属学报,1984;20:A 348
13 董元篪,彭(忄育)强,李丽芬,朱元凯,魏寿昆.全国第五届冶金物化年会论文集(上册),1984:217 |
|