| Cr系白口铸铁的磨损与断裂特性 |
| 方亮;饶启昌;周庆德 |
| 西安交通大学;西安交通大学;西安交通大学 |
|
| ABRASIVE WEAR RESISTANCE OF Cr-FAMILY WHITE CAST IRONS |
| by FANG Liang; RAO Qichang; ZHOU Qingde (Department of Mechanical Engineering; Xi'an Jiaotong University) (Manuscript received 11 August; 1985; revised manuscript 26 April; 1986) |
引用本文:
方亮;饶启昌;周庆德. Cr系白口铸铁的磨损与断裂特性[J]. 金属学报, 1987, 23(6): 575-580.
,
,
.
ABRASIVE WEAR RESISTANCE OF Cr-FAMILY WHITE CAST IRONS[J]. Acta Metall Sin, 1987, 23(6): 575-580.
1 Watson J D, Mutton P J, Sarse I R. Met Forum, 1980; 3(1) : 74-88 2 Gundlach R. B. Wear, 1978; 46: 97-108 3 Borik F. Met Eng Q, 1972; 12(2) : 33-39 4 Zum Gahr K-H, Eldis G T. Wear, 1980; 64: 175-194 5 Zum Gahr K-H. Metall Trans, 1980; 114(4) : 613-620 6 Maratray F. Factors Affecting the Structure of Chromium and Chromium-Moly-bdenum White Irons, Paris: Climax Molybdenum S A, 1971 7 Richardson R C D. Wear, 1968; 11(4) : 245-275 8 Xing J T, Lu W H, Wang X T. Wear of Materials, Int Conf on Wear of Materials, New York: ASME, 1983: 45-6 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|