铌单晶循环变形过程中的表面形变带 |
林栋梁;吴建生 |
上海交通大学;教授;上海交通大学 |
|
DEFORMATION BANDS ON SURFACE OF NIOBIUM SINGLE CRYSTALS DURING CYCLIC DEFORMATION |
LIN Dongliang (T. L. Lin)Professar;Dept.of Materials Science.Shanghai Jiaotong University;WU Jiansheng Shanghai Jiaotong University |
引用本文:
林栋梁;吴建生. 铌单晶循环变形过程中的表面形变带[J]. 金属学报, 1988, 24(2): 76-83.
,
.
DEFORMATION BANDS ON SURFACE OF NIOBIUM SINGLE CRYSTALS DURING CYCLIC DEFORMATION[J]. Acta Metall Sin, 1988, 24(2): 76-83.
1 Saletore M, Taggart R. Mater Sce Eng, 1978; 36: 259 2 Mughrabi H, Herz K, Stark X. Int J Fract, 1981; 17: 193 3 Lin Dongliang, Wu Jiansheng, Chen Xianfeng. Mater Sci Eng, 1987; 85: 19 4 吴建生.博士学位论文.上海交通大学,1985 5 Orowan E. Nature (London), 1942; 149: 643 6 A.塞格,张宏图译.晶体的范性及其理论.北京:科学出版社,1963:121 7 Crocker A G, Abell J S. Phil Mag, 1976; 33: 305 8 Guiu P, Pratt P L. Phys Status Solidi, 1966; 15: 539 9 Keh A S. Phil Mag, 1965; 12: 9 10 Duesbery M S, Foxall P A. Phil Mag, 1969; 20: 719 11 Flewitt P E J, Crocker A G. Phil Mag, 1976; 34: 877 12 Anglada M, Guiu F. Phil Mag A, 1981; 44: 433 13 Doner M, Diprimio J C, Salkovitz E I. Acta Metall, 1973; 21: 1547 14 Cotrell A H,葛庭燧译.晶体中的范性流变.北京:科学出版社,1960:174 15 冯端,王业宁,丘第荣.金属物理,下册.北京:科学出版社,1975:647 16 Hirsch P B. Prog Met Phys, 1956; 6: 236 17 Tapetado E G, Loretto M H. Phil Mag, 1974; 30: 30 18 Kuhlmann-Wilsdorf D. Phys Status Solidi (a), 1978: 47: 639 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|