PrCl_3-NaCl-LiCl三元系相图的测定 |
乔芝郁;王明生;郑朝贵;段淑贞 |
北京科技大学;北京科技大学;北京大学化学系;北京科技大学 |
|
DETERMINATION OF PrCl_3-NaCl-LiCl PHASE DIAGRAM |
QIAO Zhiyu;WANG Mingsheng;ZHENG Chaogui;DUAN Shuzhen University of Science and Technology Beijing Peking University; Beijing |
引用本文:
乔芝郁;王明生;郑朝贵;段淑贞. PrCl_3-NaCl-LiCl三元系相图的测定[J]. 金属学报, 1989, 25(4): 94-99.
,
,
,
.
DETERMINATION OF PrCl_3-NaCl-LiCl PHASE DIAGRAM[J]. Acta Metall Sin, 1989, 25(4): 94-99.
1 #12 2 郑朝贵,靳军,乔芝郁,叶于浦.中国稀土学报,1989;7(1) : 81 3 #12 4 #12 5 #12 6 郑朝贵,徐征,黄竹山,乔芝郁,叶于浦.无机化学,1988;4(4) ;134 7 服部豪夫,池沢秀男,平野亮一,持永纯一.日本化学会志,1982;126(6) :952 8 #12 9 苏勉曾,李根培.化学通报,1979;(4) :34 10 乔芝,郁王明生,郑朝贵,段淑贞.Jour al of The Chinese Rare Earth Society(English Edition),1990;7(2) : 11 Cullity B D. Elements of XR ay Diffraction, Reading Mass.: Addison-Wesley, 1956: 345 |
|