| 合金成分及弥散相对Al-Mg-Si合金疲劳断口形貌的影响 |
| 蒋大鸣;洪班德;雷廷权 |
| 哈尔滨工业大学分析测试中心;哈尔滨工业大学;哈尔滨工业大学 |
|
| INFLUENCE OF COMPOSITION AND DISPERSOID ON FATIGUE FRACTURE BEHAVIOUR OF Al-Mg-Si ALLOYS |
| JIANG Daming;HONG Bande;LEI Tingquan Harbin Institute of Technology |
引用本文:
蒋大鸣;洪班德;雷廷权. 合金成分及弥散相对Al-Mg-Si合金疲劳断口形貌的影响[J]. 金属学报, 1990, 26(5): 76-78.
,
,
.
INFLUENCE OF COMPOSITION AND DISPERSOID ON FATIGUE FRACTURE BEHAVIOUR OF Al-Mg-Si ALLOYS[J]. Acta Metall Sin, 1990, 26(5): 76-78.
1 Edwards L, Busby A K, Martin J W. Mater Sci Technol, 1986; 2: 823 2 Busby A K, Edwards L, Martin J W. Mater Sci Technol, 1986; 2: 363 3 Ludtka G M, Laughlin D E. Metall Trans, 1982; 13A: 411 4 Nix K J, Flower H M. Acta Metall, 1982; 30: 1549 5 Hornbogen E, Zum Gahr K-H. Acta Metall, 1976; 24: 581 |
|