非晶态合金的结构弛豫过程 |
刘军民;水嘉鹏 |
中山大学;中国科学院固体物理研究所 |
|
STRUCTURE RELAXATION OF AMORPHOUS ALLOYS |
LIU Junmin(Department of Physics; Zhongshan University; Guangzhou 510275);SHUI Jiapeng(Institute of Solid State Physics; Chinese Academy of Sciences; Hefei230031)(Manuscript received 1994-04-15) |
引用本文:
刘军民;水嘉鹏. 非晶态合金的结构弛豫过程[J]. 金属学报, 1995, 31(19): 318-323.
,
.
STRUCTURE RELAXATION OF AMORPHOUS ALLOYS[J]. Acta Metall Sin, 1995, 31(19): 318-323.