Please wait a minute...
金属学报  2022, Vol. 58 Issue (6): 792-798    DOI: 10.11900/0412.1961.2021.00001
  研究论文 本期目录 | 过刊浏览 |
金属Rb纳米溶胶的超声乳化制备及点火特性
郭雨静1,2, 鲍皓明1(), 符浩1,2, 张洪文1, 李文宏3, 蔡伟平1,2
1.中国科学院合肥物质科学研究院 固体物理研究所 合肥 230031
2.中国科学技术大学 研究生院科学岛分院 合肥 230026
3.河北铷铯科技有限公司 承德 063000
Ultrasonic Emulsification Preparation of Metallic Rubidium Sol and Its Ignition Performance
GUO Yujing1,2, BAO Haoming1(), FU Hao1,2, ZHANG Hongwen1, LI Wenhong3, CAI Weiping1,2
1.Institute of Solid State Physics, Hefei Institutes of Physical Science, Chinese Academy of Sciences, Hefei 230031, China
2.Graduate School of Science Island, University of Science and Technology of China, Hefei 230026, China
3.Hebei Rubidium Cesium Technology Co. Ltd., Chengde 063000, China
引用本文:

郭雨静, 鲍皓明, 符浩, 张洪文, 李文宏, 蔡伟平. 金属Rb纳米溶胶的超声乳化制备及点火特性[J]. 金属学报, 2022, 58(6): 792-798.
Yujing GUO, Haoming BAO, Hao FU, Hongwen ZHANG, Wenhong LI, Weiping CAI. Ultrasonic Emulsification Preparation of Metallic Rubidium Sol and Its Ignition Performance[J]. Acta Metall Sin, 2022, 58(6): 792-798.

全文: PDF(1815 KB)   HTML
摘要: 

基于Rb的低熔点特点,提出了固/液转变+超声分散的纳米化策略,即:将熔化的液态Rb置于特定介质(甲苯)中进行超声乳化,进而冷却凝固形成固态纳米颗粒以实现其纳米化。通过这种策略,成功获得了分散在甲苯里的Rb纳米颗粒。这些Rb纳米颗粒呈近球形,平均粒径约为45 nm。金属Rb纳米颗粒的尺寸可通过调节超声功率进行控制。随着超声功率的降低,颗粒的平均粒径增加。当超声功率降至320和240 W时,平均粒径分别增加至55和70 nm。金属Rb纳米颗粒具有良好的点火作用,可实现有机物甲苯在显著低于其着火点的温度下(如120℃)快速引燃(点火时间小于1 s),且随着温度的升高,甲苯的点火时间变短。当温度为250℃时,可在0.25 s内点燃甲苯。本工作不仅为金属Rb的纳米化提供了新的途径,而且还可望为新型含能材料及点火器件的设计提供新思路与依据。

关键词 : Rb纳米颗粒,  溶胶,  超声乳化,  点火特性    
Abstract:

Metallic rubidium (Rb) has great potential in various fields, such as energy, catalysis, and medical treatment. Fragmenting bulk Rb to the nanoscale is essential for its efficient application in these fields. However, as an alkali metal with a high chemical activity, Rb reacts violently with trace water, oxygen, and others; thus, preparing nanosized Rb is challenging. This study proposes a sample solid-liquid transformation and ultrasonic dispersion method to prepare Rb nanoparticles (NPs) utilizing Rb's low melting point. This method uses the ultrasonic emulsification of liquid Rb in a specific liquid (toluene) to form a colloidal Rb solution. Typically prepared Rb NPs are nearly spherical with an average size of approximately 45 nm. Further, the average size increases with a decrease in ultrasonic power. When the ultrasonic power falls to 320 and 240 W, the average NP size rises to 55 and 70 nm, respectively, demonstrating good controllability of the proposed method. Further experiments demonstrated that Rb NPs can ignite toluene at relatively low temperatures (say 120oC) within 1 s. When the temperature is up to 250oC, toluene can be ignited in 0.25 s. This study not only provides a new method for synthesizing Rb NPs but also offers new opportunities for novel energy-containing materials and ignition devices.

Key words: rubidium nanoparticle    sol    ultrasonic emulsification    ignition performance
收稿日期: 2021-01-05     
ZTFLH:  O611.4  
基金资助:河北省重点研发计划项目(19211002D)
作者简介: 郭雨静,女,1997年生,硕士生
图1  固/液转变+超声分散法制备Rb纳米溶胶的示意图
图2  所制备的Rb溶胶的光学吸收谱、溶胶装在样品瓶中光学照片及稀释10倍后的Tyndall效应
图3  所制备的Rb溶胶中产物的表征
图4  不同超声功率下获得的溶胶的光学吸收谱、溶胶中产物的TEM像及粒径统计
图5  Rb纳米溶胶的形成过程示意图
图6  将300 μL的甲苯/金属Rb纳米溶胶置于120℃的陶瓷舟中不同时间的点火特性
图7  金属Rb纳米溶胶在不同温度的点火时间
图8  在120℃陶瓷舟中的溶胶液膜的形态演变及引燃示意图
1 Tan Y N, Liu Y. Properties and research progress of rubidium and its compounds [J]. Chin. J. Nonferrous Met., 2017, 27: 272
doi: 10.1016/S1003-6326(17)60031-1
1 谭彦妮, 刘 咏. 铷及含铷材料的性能与应用研究进展 [J]. 中国有色金属学报, 2017, 27: 272
2 Cui Y J, Liu Y, Yang B. The design of high precision time reference measurement system based on rubidium disciplined crystal oscillator and double TDC GP2 [J]. Chin. J. Electron Dev., 2017, 40: 1072
2 崔永俊, 刘 阳, 杨 兵. 基于铷原子钟和双TDC-GP2的高精度时间基准测量系统的设计 [J]. 电子器件, 2017, 40: 1072
3 Chang S M, Guo Y. Influences of alkali metal Rb doped Mn as catalyst on catalytic combustion activity of soot particle [J]. China Adhes., 2017, 26(5): 25
3 常三毛, 郭 耘. 碱金属Rb掺锰对碳烟颗粒催化燃烧活性的影响 [J]. 中国胶粘剂, 2017, 26(5): 25
4 Yang Y, Zhang Y, Guo Q, et al. Effect of extracellular potassium on the activity of distal renal tubule in mice [J]. J. Shanghai Jiaotong Univ. (Med. Sci.), 2019, 39(9): 85
4 杨 阳, 张 娅, 郭 琴 等. 细胞外钾对小鼠远端肾小管离子通道活性的影响 [J]. 上海交通大学学报(医学版), 2019, 39(9): 985
5 Qian J M, Li X X, Huang H Y. Properties of nanometer materials and its preparing methods [J]. New Chem. Mater., 2001, 29(7): 1
5 钱军民, 李旭祥, 黄海燕. 纳米材料的性质及其制备方法 [J]. 化工新型材料, 2001, 29(7): 1
6 Li X H, Guo S H, Su J, et al. Efficient raman enhancement in molybdenum disulfide by tuning the interlayer spacing [J]. ACS Appl. Mater. Interfaces, 2020, 12: 28474
doi: 10.1021/acsami.0c04151
7 Zhu M Y, Chen Q, Tong W J, et al. Preparation and application of Fe3O4 nanomaterials [J]. Prog. Chem., 2017, 29: 1366
7 朱脉勇, 陈 齐, 童文杰 等. 四氧化三铁纳米材料的制备与应用 [J]. 化学进展, 2017, 29: 1366
doi: 10.7536/PC170559
8 Yang M Q, Ji Y H, Liang Q, et al. Preparation, doping modulation and field emission properties of square-shaped GaN nanowires [J]. Acta Phys. Sin., 2020, 69: 167805
doi: 10.7498/aps.69.20200445
8 杨孟骐, 姬宇航, 梁 琦 等. 四方结构GaN纳米线制备、掺杂调控及其场发射性能研究 [J]. 物理学报, 2020, 69: 167805
9 Sun Q S, Ni C L, Yu Y C, et al. Design principle of all-inorganic halide perovskite-related nanocrystals [J]. J. Mater. Chem., 2018, 6C: 12484
10 Liu H G, Tian R Y, Jiang Y, et al. On the drastically improved performance of Fe-doped LiMn2O4 nanoparticles prepared by a facile solution-gelation route [J]. Electrochim. Acta, 2015, 180: 138
doi: 10.1016/j.electacta.2015.08.123
11 Xu X Y, Wang Y L, Wang R, et al. Creating carbon-oxygen bonds over TiO2 nanofibers for synergistic benefits of visible-light response and charge separation toward photocatalysis [J]. Adv. Mater. Interfaces, 2017, 4: 1600795
doi: 10.1002/admi.201600795
12 Bozlee B, Lian B, Kahn J, et al. Characterization of alkali-metal sols in diethyl ether. Visible extinction and surface-enhanced Raman spectra [J]. Chem. Phys. Lett., 1992, 196: 437
doi: 10.1016/0009-2614(92)85717-O
13 Bozlee B, Clark S, Marr C, et al. Characterization and surface-enhanced Raman spectroscopy of alkali metal sols [J]. J. Raman Spectrosc., 1996, 27: 75
doi: 10.1002/(SICI)1097-4555(199601)27:1<75::AID-JRS929>3.0.CO;2-E
14 Roginsky S, Schalnikoff A. A new method of production of colloid solutions [J]. Kolloid Z., 1927, 43: 67
doi: 10.1007/BF01751491
15 Tomaschewsky N. Concerning the manufacture of colloids from the condensation method of molecular rays [J]. Kolloid Z., 1931, 54: 79
doi: 10.1007/BF01422259
16 Modarres-Gheisari S M M, Gavagsaz-Ghoachani R, Malaki M, et al. Ultrasonic nano-emulsification—A review [J]. Ultrason. Sonochem., 2019, 52: 88
doi: S1350-4177(18)31269-0 pmid: 30482437
17 Baissac L, Buron C C, Hallez L, et al. Synthesis of sub-micronic and nanometric PMMA particles via emulsion polymerization assisted by ultrasound: Process flow sheet and characterization [J]. Ultrason. Sonochem., 2018, 40: 183
doi: S1350-4177(17)30120-7 pmid: 28359634
18 Behbahani E S, Ghaedi M, Abbaspour M, et al. Optimization and characterization of ultrasound assisted preparation of curcumin-loaded solid lipid nanoparticles: Application of central composite design, thermal analysis and X-ray diffraction techniques [J]. Ultrason. Sonochem., 2017, 38: 271
doi: S1350-4177(17)30106-2 pmid: 28633826
19 Jia Q P, Ma Z L, Han B, et al. Effects on SPR of Au/TiO2 by preparation methods [J]. J. Hebei Univ. (Nat. Sci. Ed.), 2020, 40: 385
19 贾群鹏, 马志领, 韩 冰 等. Au/TiO2的制备方法对其SPR的影响 [J]. 河北大学学报(自然科学版), 2020, 40: 385
20 Zhu W Z, Liu Y Q, Meng G. Preparation and characterization of nano-gold particles by seeding method [J]. Chin. J. Veter. Med., 2019, 55(10): 33
20 朱文壮, 刘轶群, 孟 赓. 纳米金颗粒的晶种法制备及表征 [J]. 中国兽医杂志, 2019, 55(10): 33
21 Li C X, Wang Z H. Applications of ultrasound in preparation of nanosized materials [J]. Chemistry, 2001, 64: 268
21 李春喜, 王子镐. 超声技术在纳米材料制备中的应用 [J]. 化学通报, 2001, 64: 268
22 Vyas N, Manmi K, Wang Q X, et al. Which parameters affect biofilm removal with acoustic cavitation? A review [J]. Ultrasound Med. Biol., 2019, 45: 1044
doi: 10.1016/j.ultrasmedbio.2019.01.002
23 Jiang R P. Effect rules and function mechanism of ultrasonic field on the solidification of high strength aluminum alloy [D]. Changsha: Central South University, 2014
23 蒋日鹏. 超声场对高强铝合金凝固过程的影响规律与作用机理研究 [D]. 长沙: 中南大学, 2014
24 Ma L. Mechanism for ultrasonic driving filling of liquid solder and acoustic cavitation [D]. Harbin: Harbin Institute of Technology, 2015
24 马 琳. 液态钎料超声驱动填缝机理及声空化作用研究 [D]. 哈尔滨: 哈尔滨工业大学, 2015
25 Sajjadi B, Raman A A A, Shah R S S R E, et al. Review on applicable breakup/coalescence models in turbulent liquid-liquid flows [J]. Rev. Chem. Eng., 2013, 29: 131
26 Kulawik-Pióro A, Tal-Figiel B. Influence of preparation method on size distribution of the dispersed phase of primary emulsions [J]. Chem. Eng. Technol., 2017, 40: 412
doi: 10.1002/ceat.201500746
27 Li X T, Gao X P, Li T J, et al. A experimental study of grain refinement by ultrasonic treatment during continuous casting [J]. Rare Met. Mater. Eng., 2007, 36: 377
27 李新涛, 高学鹏, 李廷举 等. 连铸过程中超声细晶技术研究 [J]. 稀有金属材料与工程, 2007, 36: 377
[1] 范超, 贾清, 崔玉友, 杨锐. 基于溶胶-凝胶法的YAlO3/Ti2AlC复合涂层在干燥与热分解过程中的开裂行为研究[J]. 金属学报, 2018, 54(7): 991-998.
[2] 单麟婷, 巴德纯, 曹青, 侯雪艳, 李建昌. Ce-Cu共掺杂对SnO2薄膜光电特性的影响*[J]. 金属学报, 2014, 50(1): 95-102.
[3] 潘晓铭,吴俊升,肖葵,高书君,裴礼鸿,田然,李晓刚. 铝合金表面缓蚀自修复疏水性膜层的制备与表征[J]. 金属学报, 2013, 49(9): 1113-1120.
[4] 高茜 孙本哲 祁阳 齐连仲. 溶胶--凝胶法制备的Zn1-xCoxO晶体粉末的结构和磁性行为[J]. 金属学报, 2011, 47(3): 337-343.
[5] 厉英 马北越 王臻明 姜茂发. Na1.4Co2O4基热电材料的溶胶-凝胶法制备及表征[J]. 金属学报, 2011, 47(1): 109-114.
[6] 蔡辉 王菲 王亚平 宋晓平 丁秉钧. Si粉表面溶胶-凝胶预处理制备Cu/Si复合材料[J]. 金属学报, 2009, 45(10): 1261-1266.
[7] 李坤; 裴志亮; 宫骏; 石南林; 孙超 . 碳纤维表面SiO2涂层的制备及其在镁基复合材料中的应用[J]. 金属学报, 2007, 43(12): 1282-1286 .
[8] 黄辉; 朱明伟; 宫骏; 孙超; 姜辛 . 溶剂、溶胶稳定剂和热处理对溶胶--凝胶法制备的ZnO薄膜微观结构的影响[J]. 金属学报, 2007, 43(10): 1043-1047 .
[9] 周宏明; 易丹青; 余志明; 肖来荣; 李荐; 王斌 . 溶胶-凝胶法制备的ZnO∶Al薄膜的微观结构及光学、电学性能[J]. 金属学报, 2006, 42(5): 505-510 .
[10] 征茂平; 金燕苹; 吴桢干; 金国良; 顾明元 . Sol-gel法制备TiO2/PVP纳米复合材料及其表征[J]. 金属学报, 1999, 35(11): 1224-1228 .
[11] 余圣甫;刘顺洪;谢明立;李志远;王杰. 非晶态药芯焊丝药芯材料[J]. 金属学报, 1998, 34(1): 91-94.
[12] 曾庆冰. 溶胶-凝胶法TiO_2涂层碳纤维增强铝基复合材料[J]. 金属学报, 1997, 33(9): 1002-1008.