| 冶金型气孔对熔化焊接7020铝合金疲劳行为的影响 |
宋哲1, 吴圣川1( ), 胡雅楠1, 康国政1, 付亚楠2, 肖体乔2 |
1 西南交通大学牵引动力国家重点实验室 成都 610031 2 中国科学院上海应用物理研究所上海同步辐射光源 上海 201204 |
|
| The Influence of Metallurgical Pores on Fatigue Behaviors of Fusion Welded AA7020 Joints |
Zhe SONG1, Shengchuan WU1( ), Yanan HU1, Guozheng KANG1, Yanan FU2, Tiqiao XIAO2 |
1 State Key Laboratory of Traction Power, Southwest Jiaotong University, Chengdu 610031, China 2 Shanghai Synchrotron Radiation Facility (SSRF), Shanghai Institute of Applied Physics, Chinese Academy of Sciences, Shanghai 201204, China |
引用本文:
宋哲, 吴圣川, 胡雅楠, 康国政, 付亚楠, 肖体乔. 冶金型气孔对熔化焊接7020铝合金疲劳行为的影响[J]. 金属学报, 2018, 54(8): 1131-1140.
Zhe SONG,
Shengchuan WU,
Yanan HU,
Guozheng KANG,
Yanan FU,
Tiqiao XIAO.
The Influence of Metallurgical Pores on Fatigue Behaviors of Fusion Welded AA7020 Joints[J]. Acta Metall Sin, 2018, 54(8): 1131-1140.
| [1] | Yu C, Wu S C, Hu Y N, et al.Three-dimensional imaging of gas pores in fusion welded Al alloys by synchrotron radiation X-ray microtomography[J]. Acta Metall. Sin., 2015, 51: 159(喻程, 吴圣川, 胡雅楠等. 铝合金熔焊微气孔的三维同步辐射X射线成像[J]. 金属学报, 2015, 51: 159) | | [2] | Zhang J, Lei Z, Wang X Y.Weld hot crack analysis of 6005A aluminum alloy profile for high-speed train[J]. Trans. China Weld. Inst., 2012, 33(8): 60(张健, 雷振, 王旭友. 高速列车6005A铝合金型材焊接热裂纹分析[J]. 焊接学报, 2012, 33(8): 60) | | [3] | Wu S C, Zhu Z T, Li X W.Laser Welding of Aluminum Alloys and the Performance Evaluation [M]. Beijing: National Defense Industry Press, 2014: 18(吴圣川, 朱宗涛, 李向伟. 铝合金的激光焊接及性能评价 [M]. 北京: 国防工业出版社, 2014: 18) | | [4] | Vanderesse N, Maire é, Chabod A, et al.Microtomographic study and finite element analysis of the porosity harmfulness in a cast aluminium alloy[J]. Int. J. Fatigue, 2011, 33: 1514 | | [5] | Buffière J Y, Savelli S, Jouneau P H, et al.Experimental study of porosity and its relation to fatigue mechanisms of model Al-Si7-Mg0.3 cast Al alloys[J]. Mater. Sci. Eng., 2001, A316: 115 | | [6] | Wang Q G, Apelian D, Lados D A.Fatigue behavior of A356-T6 aluminum cast alloys. Part I. Effect of casting defects[J]. J. Light Met., 2001, 1: 73 | | [7] | Zhang B, Chen W, Poirier D R.Effect of solidification cooling rate on the fatigue life of A356.2-T6 cast aluminium alloy[J]. Fatigue Fract. Eng. Mater. Struct., 2000, 23: 417 | | [8] | Toda H, Masuda S, Batres R, et al.Statistical assessment of fatigue crack initiation from sub-surface hydrogen micropores in high-quality die-cast aluminum[J]. Acta Mater., 2011, 59: 4990 | | [9] | Wu S C, Xiao T Q, Withers P J.The imaging of failure in structural materials by synchrotron radiation X-ray microtomography[J]. Eng. Fract. Mech., 2017, 182: 127 | | [10] | Brochu M, Verreman Y, Ajersch F, et al.High cycle fatigue strength of permanent mold and rheocast aluminum 357 alloy[J]. Int. J. Fatigue, 2010, 32: 1233 | | [11] | Serrano-Munoz I, Buffiere J Y, Mokso R, et al.Location, location & size: Defects close to surfaces dominate fatigue crack initiation[J]. Sci. Rep., 2017, 7: 45239 | | [12] | Serrano-Munoz I, Buffiere J Y, Verdu C, et al.Influence of surface and internal casting defects on the fatigue behaviour of A357-T6 cast aluminium alloy[J]. Int. J. Fatigue, 2016, 82: 361 | | [13] | Mu P, Nadot Y, Nadot-Martin C, et al.Influence of casting defects on the fatigue behavior of cast aluminum AS7G06-T6[J]. Int. J. Fatigue, 2014, 63: 97 | | [14] | Wu S C, Hu Y N, Fu Y N, et al.Study on fatigue cracking of welded aluminum alloys via in situ synchrotron radiation X-ray microtomography[J]. Trans. China Weld. Inst., 2015, 36(12): 5(吴圣川, 胡雅楠, 付亚楠等. 铝合金焊缝疲劳开裂的原位同步辐射X射线成像[J]. 焊接学报, 2015, 36(12): 5) | | [15] | Wu S C, Yu C, Yu P S, et al.Corner fatigue cracking behavior of hybrid laser AA7020 welds by synchrotron X-ray computed microtomography[J]. Mater. Sci. Eng., 2016, A651: 604 | | [16] | Wu S C, Yu C, Zhang W H, et al.Porosity induced fatigue damage of laser welded 7075-T6 joints investigated via synchrotron X-ray microtomography[J]. Sci. Technol. Weld. Join., 2015, 20: 11 | | [17] | Yadollahi A, Shamsaei N.Additive manufacturing of fatigue resistant materials: Challenges and opportunities[J]. Int. J. Fatigue, 2017, 98: 14 | | [18] | Hu Y N, Wu S C, Zhang S Q, et al.Three-dimensional X-ray micro-tomography based microstructure and mechanical performance of hybrid laser welded AA7020[J]. Chin. J. Lasers, 2016, 43: 84(胡雅楠, 吴圣川, 张思齐等. 基于三维X射线成像的激光复合焊接7020铝合金的组织与力学特性演变[J]. 中国激光, 2016, 43: 84) | | [19] | Ferrié E, Buffière J Y, Ludwig W.3D characterisation of the nucleation of a short fatigue crack at a pore in a cast Al alloy using high resolution synchrotron microtomography[J]. Int. J. Fatigue, 2005, 27: 1215 | | [20] | Murakami Y.Metal Fatigue: Effects of Small Defects and Nonmetallic Inclusions[M]. Oxford: Elsevier, 2002: 44 | | [21] | Xu Z Q, Wen W, Zhai T G.Effects of pore position in depth on stress/strain concentration and fatigue crack initiation[J]. Metall. Mater. Trans., 2012, 43A: 2763 | | [22] | Tammas-Williams S, Withers P J, Todd I, et al.The influence of porosity on fatigue crack initiation in additively manufactured titanium components[J]. Sci. Rep., 2017, 7: 7308 | | [23] | Li P, Lee P D, Maijer D M, et al.Quantification of the interaction within defect populations on fatigue behavior in an aluminum alloy[J]. Acta Mater., 2009, 57: 3539 | | [24] | Walker K.The effect of stress ratio during crack propagation and fatigue for 2024-T3 and 7075-T6 aluminum [A]. Effects of Environment and Complex Load History on Fatigue Life[C]. West Conshohocken, PA: ASTM, 1970, 462: 1 | | [25] | Dowling N E, Calhoun C A, Arcari A.Mean stress effects in stress-life fatigue and the Walker equation[J]. Fatigue Fract. Eng. Mater. Struct., 2009, 32: 163 | | [26] | Borbély A, Mughrabi H, Eisenmeier G, et al.A finite element modelling study of strain localization in the vicinity of near-surface cavities as a cause of subsurface fatigue crack initiation[J]. Int. J. Fract., 2002, 115: 227 | | [27] | Dezecot S, Maurel V, Buffiere J Y, et al.3D characterization and modeling of low cycle fatigue damage mechanisms at high temperature in a cast aluminum alloy[J]. Acta Mater., 2017, 123: 24 | | [28] | Gerard D A, Koss D A.The influence of porosity on short fatigue crack growth at large strain amplitudes[J]. Int. J. Fatigue, 1991, 13: 345 | | [29] | Mo D F, He G Q, Hu Z F, et al.Effect of porosity on fatigue property in aluminum cast alloys[J]. J. Mater. Eng., 2010, (7): 92(莫德锋, 何国求, 胡正飞等. 孔洞对铸造铝合金疲劳性能的影响[J]. 材料工程, 2010, (7): 92) | | [30] | Paris P C, Erdogan F.A critical analysis of crack propagation laws[J]. J. Basic Eng., 1963, 85: 528 | | [31] | Zhang H, Toda H, Hara H, et al.Three-dimensional visualization of the interaction between fatigue crack and micropores in an aluminum alloy using synchrotron X-ray microtomography[J]. Metall. Mater. Trans., 2007, 38A: 1774 | | [32] | Tsay L W, Shan Y P, Chao Y H, et al.The influence of porosity on the fatigue crack growth behavior of Ti-6Al-4V laser welds[J]. J. Mater. Sci., 2006, 41: 7498 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|