| 中厚板表层超细晶对止裂性能的影响 |
马江南1,王瑞珍2( ),杨才福2,查小琴1,张利娟1 |
1 洛阳船舶材料研究所 洛阳 471023 2 钢铁研究总院工程用钢所 北京 100081 |
|
| Effect of Surface Layer with Ultrafine Grains on Crack Arrestability of Heavy Plate |
Jiangnan MA1,Ruizhen WANG2( ),Caifu YANG2,Xiaoqin ZHA1,Lijuan ZHANG1 |
1 Luoyang Ship Material Research Institute, Luoyang 471023, China 2 Department of Engineering Steels, Central Iron and Steel Research Institute, Beijing 100081, China |
引用本文:
马江南,王瑞珍,杨才福,查小琴,张利娟. 中厚板表层超细晶对止裂性能的影响[J]. 金属学报, 2017, 53(5): 549-558.
Jiangnan MA,
Ruizhen WANG,
Caifu YANG,
Xiaoqin ZHA,
Lijuan ZHANG.
Effect of Surface Layer with Ultrafine Grains on Crack Arrestability of Heavy Plate[J]. Acta Metall Sin, 2017, 53(5): 549-558.
| [1] | Weng Y Q, Yang C F, Shang C J.State-of-the-art and development trends of HSLA steels in China[J]. Iron Steel, 2011, 46(9): 1 | | [1] | (翁宇庆, 杨才福, 尚成嘉. 低合金钢在中国的发展现状与趋势[J]. 钢铁, 2011, 46(9): 1) | | [2] | Komizo Y I.Status & prospects of shipbuilding steel and its weldability[J]. Trans. JWRI, 2007, 36: 1 | | [3] | Ishikawa T, Nomiyama Y, Yoshikawa H, et al.Ultra-high crack-arresting steel plate (HIAREST) with super-refined grains in surface layers[J]. Nippon Steel Tech. Rep., 1997, 75(11): 31 | | [4] | Yao L D, Li Z G, Zhang P J.Research on ultra-fine grain and ultra-high toughness steel plate[J]. Iron Steel Vanadium Titanium, 2005, 26(1): 20 | | [4] | (姚连登, 李自刚, 张丕军. 超细晶粒及超高韧性厚板的研究[J]. 钢铁钒钛, 2005, 26(1): 20) | | [5] | Mabuchi H, Hasegawa T, Ishikawa T.Metallurgical features of steel plates with ultra fine grains in surface layers and their formation mechanism[J]. ISIJ Int., 1999, 39: 477 | | [6] | Zhao S X, Yao L D, Zhao X T.Development of heavy plate with ultra fine grained surface layer[J]. World Iron Steel, 2009, (5): 18 | | [6] | (赵四新, 姚连登, 赵小婷. 表层超细晶厚钢板的研制[J]. 世界钢铁, 2009, (5): 18) | | [7] | Du H J, Li C, Zhao D W, et al.Development of Nb microalloyed low carbon steel plate with ultra-fine grains in surface layer[J]. J. Mech. Eng., 2011, 47(2): 58 | | [7] | (杜海军, 栗春, 赵德文等. Nb微合金低碳钢表层超细晶中厚板的研制[J]. 机械工程学报, 2011, 47(2): 58) | | [8] | Ma J N, Yang C F, Wang R Z.Microstructure transformation and ferrite dynamic recrystallization behavior of microalloyed steel during temperature-reversion deforming[J]. J. Mater. Eng., 2015, 43(11): 24(马江南, 杨才福, 王瑞珍. 微合金钢回温变形时的组织转变和铁素体动态再结晶行为 [J]. 材料工程, 2015, 43(11): 24) | | [9] | Ishikawa T, Mabuchi H, Hasegawa T, et al.High crack arrestability-endowed steel plate with surface-layer of ultra fine grain microstructure[J]. Tetsu Hagané, 1999, 85: 544 | | [9] | (石川忠, 間渕秀里, 長谷川俊永など. 脆性き裂伝播停止性能の優れた表層超細粒鋼板[J]. 鉄と鋼, 1999, 85: 544) | | [10] | He Q Z, Li Z N.Engineering Fracture Mechanics [M]. Beijing: Beijing University of Aeronautics and Astronautics Press, 1993: 55(何庆芝, 郦正能. 工程断裂力学 [M]. 北京: 北京航空航天大学出版社, 1993: 55) | | [11] | Ma J N, Yang C F, Wang R Z.Numerical simulation of temperature field and experiment during temperature-reverting rolling process of heavy steel plate[J]. Trans. Mater. Heat Treat., 2015, 36(3): 220 | | [11] | (马江南, 杨才福, 王瑞珍. 中厚钢板回温轧制温度场的数值模拟和试验[J]. 材料热处理学报, 2015, 36(3): 220) | | [12] | Wang R Z, Lei T C.Dynamic recrystallization of ferrite in a low carbon steel during hot rolling in the (F+A) two-phase range[J]. Scr. Metall. Mater., 1994, 31: 1193 | | [13] | Hales S J, Mcnelley T R.Microstructural evolution by continuous recrystallization in a superplastic Al-Mg alloy[J]. Acta Metall., 1988, 36: 1229 | | [14] | Yang C F, Zhang Y Q, Liu T J.Low temperature impact fracture behavior of 10Ni5CrMoV steel[J]. Dev. Appl. Mater., 1997, 12(6): 2 | | [14] | (杨才福, 张永权, 刘天军. 10Ni5CrMoV钢低温冲击断裂行为研究[J]. 材料开发与应用, 1997, 12(6): 2) | | [15] | Liu D Y, Xu H, Yang K, et al.Effect of bainite/martensite mixed microstructure on the strength and toughness of low carbon alloy steels[J]. Acta Metall. Sin., 2004, 40: 882 | | [15] | (刘东雨, 徐鸿, 杨昆等. 贝氏体/马氏体复相组织对低碳合金钢强韧性的影响[J]. 金属学报, 2004, 40: 882) | | [16] | Zhang Y Q, Liu T J, Yang C F.Effect of melting methods on low temperature brittleness of steel 10CrSiNiCu[J]. J. Iron Steel Res., 1998, 10(5): 36 | | [16] | (张永权, 刘天军, 杨才福. 不同冶炼方法对10CrSiNiCu钢低温脆性的影响[J]. 钢铁研究学报, 1998, 10(5): 36) | | [17] | Liu D S, Cheng B G, Luo M.Microstructure and impact fracture behaviour of HAZ of F460 heavy ship plate with high strength and toughness[J]. Acta Metall. Sin., 2011, 47: 1233 | | [17] | (刘东升, 程丙贵, 罗咪. F460高强韧厚船板焊接热影响区的组织和冲击断裂行为[J]. 金属学报, 2011, 47: 1233) | | [18] | Hashemi S H.Apportion of Charpy energy in API 5L grade X70 pipeline steel[J]. Int. J. Pressure Vessels Piping, 2008, 85: 879 | | [19] | Deng W, Gao X H, Qin X M, et al.Impact fracture behavior of X80 pipeline steel[J]. Acta Metall. Sin., 2010, 46: 533 | | [19] | (邓伟, 高秀华, 秦小梅等. X80管线钢的冲击断裂行为[J]. 金属学报, 2010, 46: 533) | | [20] | Liu D S, Cheng B G, Luo M.Effect of heat-treatment processes on microstructure and properties of a NV-F690 shipbuilding plate steel[J]. Trans. Mater. Heat Treat., 2011, 32(9): 125 | | [20] | (刘东升, 程丙贵, 罗咪. 热处理工艺对NV-F690船板钢组织和性能的影响[J]. 材料热处理学报, 2011, 32(9): 125) | | [21] | Yang P, Fu Y Y, Cui F E, et al.Orientational inspection of ferrite grains during strain enhanced transformation in plain carbon steel Q235[J]. Acta Metall. Sin., 2001, 37: 900 | | [21] | (杨平, 傅云义, 崔凤娥等. Q235碳素钢应变强化相变过程中铁素体晶粒取向分析[J]. 金属学报, 2001, 37: 900) | | [22] | Lv Q G, Chen G N, Zhou J C, et al.Textures in hot rolled steel sheet[J]. Iron Steel Vanadium Titanium, 2001, 22(2): 1 | | [22] | (吕庆功, 陈光南, 周家琮等. 热轧钢板的织构[J]. 钢铁钒钛, 2001, 22(2): 1) | | [23] | Liu D S, Cheng B G, Luo M.F460 heavy steel plates for offshore structure and shipbuilding produced by thermomechanical control process[J]. ISIJ Int., 2011, 51: 603 | | [24] | Gao G H, Zhang H, Bai B Z.Effect of tempering temperature on low temperature impact toughness of a low carbon Mn-series bainitic steel[J]. Acta Metall. Sin., 2011, 47: 513 | | [24] | (高古辉, 张寒, 白秉哲. 回火温度对Mn系低碳贝氏体钢的低温韧性的影响[J]. 金属学报, 2011, 47: 513) | | [25] | Liu D S, Li Q L, Emi T.Microstructure and mechanical properties in hot-rolled extra high-yield-strength steel plates for offshore structure and shipbuilding[J]. Metall. Mater. Trans., 2011, 42A: 1349 | | [26] | Liu Z X, Li D Z, Qiao G W.Investigation on deformation induced ferrite (a kind of martensite) transformation above Ae3 temperature in a low carbon steel[J]. Acta Metall. Sin., 2005, 41: 1127 | | [26] | (刘朝霞, 李殿中, 乔桂文. 低碳钢在Ae3温度之上的形变诱导铁素体(一种马氏体)的相变研究[J]. 金属学报, 2005, 41: 1127) |
|
|