| 在AlCl3的辅助下从LiCl-KCl-AlCl3-Nd2O3熔盐中电解提取Nd* |
薛云1,2,杨雪1,颜永得1( ),张密林1,纪德彬1,李恩雨1,韩伟1 |
1 哈尔滨工业大学金属精密热加工国家级重点实验室, 哈尔滨 150001。 2 沈阳黎明航空发动机(集团)有限责任公司, 沈阳 110043。 |
|
| ELECTROLYSIS EXTRACTION OF NEODYMIUM FROM LiCl-KCl-AlCl3-Nd2O3 MELTS WITHTHE ASSISTANCE OF AlCl3 |
Yun XUE1,2,Xue YANG1,Yongde YAN1( ),Milin ZHANG1,Debin JI1,Enyu LI1,Wei HAN1 |
1 Key Laboratory of Superlight Materials and Surface Technology, Ministry of Education, College of Materials Science and Chemical Engineering, Harbin Engineering University, Harbin 150001, China. 2 Fundamental Science on Nuclear Safety and Simulation Technology Laboratory, Harbin Engineering University, Harbin 150001, China. |
引用本文:
薛云,杨雪,颜永得,张密林,纪德彬,李恩雨,韩伟. 在AlCl3的辅助下从LiCl-KCl-AlCl3-Nd2O3熔盐中电解提取Nd*[J]. 金属学报, 2016, 52(7): 883-889.
Yun XUE,
Xue YANG,
Yongde YAN,
Milin ZHANG,
Debin JI,
Enyu LI,
Wei HAN.
ELECTROLYSIS EXTRACTION OF NEODYMIUM FROM LiCl-KCl-AlCl3-Nd2O3 MELTS WITHTHE ASSISTANCE OF AlCl3[J]. Acta Metall Sin, 2016, 52(7): 883-889.
| [1] | Gu Z M.J Nucl Radiochem, 2006; 28: 1 | | [1] | (顾忠茂. 核化学与放射化学, 2006; 28: 1) | | [2] | Zhou P D.Nucl Sci Eng, 2002; 22: 261 | | [2] | (周培德. 核科学与工程, 2002; 22: 261) | | [3] | Smolenski V, Novoselova A, Bovet A, Osipenko A, Kormilitsyn M.J Nucl Mater, 2009; 385: 184 | | [4] | Castrillejo Y, Bermejo M R, Barrado E, Barrado E, Martinez A M.Electrochim Acta, 2006; 51: 1941 | | [5] | Castrillejo Y, Bermejo M R, Barrado A I, Rardo R, Barrado E, Martinez A M.Electrochim Acta, 2005; 50: 2047 | | [6] | Bermejo M R, Gómez J, Medina J, Martinez A M, Castrillejo Y.J Electroanal Chem, 2006; 588: 253 | | [7] | Du S L, Su M Z.Acta Metall Sin, 1991; 27: 111 | | [7] | (杜森林, 苏明忠. 金属学报, 1991; 27: 111) | | [8] | Nourry C, Massot L, Chamelot P, Taxil P.J Appl Electrochem, 2009; 39: 2359 | | [9] | Taxil P, Massot L, Nourry C, Gibilaro M, Chamelot P, Cassayre L.J Fluorine Chem, 2009; 130: 94 | | [10] | Xue Y, Zhou Z P, Yan Y D, Zhang M L, Li X, Ji D B, Han W, Zhang M.Acta Phys Chim Sin, 2014; 30: 1674 | | [10] | (薛云, 周志萍, 颜永得, 张密林, 李星, 纪德彬, 韩伟, 张萌. 物理化学学报, 2014; 30: 1674) | | [11] | Xue Y, Zhou Z P, Yan Y D, Zhang M L, Li X, Ji D B, Tang H, Zhang Z J.RSC Adv, 2015; 5: 23114 | | [12] | Li X, Yan Y D, Zhang M L, Xue Y, Tang H, Zhou Z P, Yang X N, Zhang Z J.J Electrochem Soc, 2014; 161: D248 | | [13] | Zhang M L, Yang Y S, Han W, Li M, Ye K, Sun Y, Yan Y D.J Solid State Chem, 2013; 17: 2671 | | [14] | Tang H, Yan Y D, Zhang M L, Li X, Han W, Xue Y, Zhang Z J, He H.Electrochim Acta, 2013; 107: 209 | | [15] | Papatheodorou G N, Kucera G H.Inorg Chem, 1979; 18: 385 | | [16] | Xue Y, Wang Q, Yan Y D, Chen L, Zhang M L, Zhang Z J.Energy Procedia, 2013; 39: 474 | | [17] | Yan Y D, Tang H, Zhang M L, Xue Y, Han W, Cao D X, Zhang Z Z.Electrochim Acta, 2012; 59: 531 | | [18] | Wang L, Liu Y L, Liu K, Tang S L, Yuan L Y, Su L L, Chai Z F, Shi W Q.Electrochim Acta, 2014; 147: 385 | | [19] | Fukasawa K, Uehara A, Nagai T, Fujii T, Yamana H.J Nucl Mater, 2011; 414: 265 | | [20] | De Cordoba G, Laplace A, Conocar O, Lacquement J, Caravaca C.Electrochim Acta, 2008; 54: 280 | | [21] | Tang H, Pesic B.J Nucl Mater, 2015; 458: 37 | | [22] | Yan Y D, Xu Y L, Zhang M L, Xue Y, Han W, Hang Y, Chen Q, Zhang Z J.J Nucl Mater, 2013; 433: 152 | | [23] | Li X, Yan Y D, Zhang M L, Xue Y, Tang H, Zhou Z P, Yang X N, Zhang Z J.J Radioanal Nucl Chem, 2014; 299: 657 | | [24] | Yan Y D, Yang X N, Zhang M L, Li X, Wang L, Xue Y, Zhang Z J.Acta Metall Sin, 2014; 50: 989 | | [24] | (颜永得, 杨晓南, 张密林, 李星, 王丽, 薛云, 张志俭. 金属学报, 2014; 50: 989) | | [25] | Massalski T B, Murray J L, Benett L H, Baker H.Binary Alloy Phase Diagrams. Vol.1, Metals Park, Ohio: The Materials Information Company, 1986: 293 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|