| 金属连接体涂层材料MnCo2O4尖晶石的氧化动力学行为和电性能* |
张文颖1( ),李俊2,周波1 |
1 中国地质大学机械与电子信息学院, 武汉 430074
2 华中科技大学材料科学与工程学院材料成型与模具技术重点实验室, 武汉 430074 |
|
| OXIDATION KINETICS BEHAVIOR AND ELECTRICAL PROPERTY OF MnCO2O4 SPINEL AS A COATING MATERIAL FOR METALLIC INTERCONNECTS |
Wenying ZHANG1( ),Jun LI2,Bo ZHOU1 |
1 School of Mechanical Engineering and Electronic Information, China University of Geosciences, Wuhan 430074, China
2 State Key Laboratory of Materials Processing and Die&Mould Technology, School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan 430074, China |
引用本文:
张文颖, 李俊, 周波. 金属连接体涂层材料MnCo2O4尖晶石的氧化动力学行为和电性能*[J]. 金属学报, 2016, 52(3): 355-360.
Wenying ZHANG,
Jun LI,
Bo ZHOU.
OXIDATION KINETICS BEHAVIOR AND ELECTRICAL PROPERTY OF MnCO2O4 SPINEL AS A COATING MATERIAL FOR METALLIC INTERCONNECTS[J]. Acta Metall Sin, 2016, 52(3): 355-360.
| [1] | Yang Z G.Int Mater Rev, 2008; 53: 39 | | [2] | Zhu W Z, Deevi S C.Mater Res Bull, 2003; 38: 957 | | [3] | Fergus J W.Mater Sci Eng, 2005; A397: 271 | | [4] | Toji A, Uehara T.ECS Trans, 2007; 7: 2117 | | [5] | Han M F, Peng S P, Wang Z L, Yang Z B, Chen X.J Power Sources, 2007; 164: 278 | | [6] | Pu J, Li J, Hua B, Xie G Y.J Power Sources, 2006; 158: 354 | | [7] | Stanislowski M, Wessel E, Hilpert K, Markus T, Singheiser L.J Electrochem Soc, 2007; 154: A295 | | [8] | Tucker M C, Kurokawa H, Jacobson C P, De Jonghe L C, Visco S J.J Power Sources, 2006; 160: 130 | | [9] | Shaigan N, Qu W, Ivey D G, Chen W.J Power Sources, 2010; 195: 1529 | | [10] | Qu W, Li J, Ivey D G, Hill J M.J Power Sources, 2006; 157: 335 | | [11] | Oishi N, Namikawa T, Yamazaki Y.Surf Coat Technol, 2000; 132(1): 58 | | [12] | Roure S, Czerwinski F, Petric A.Oxid Met, 1994; 42(1~2): 75 | | [13] | Johnson C, Gemmen R, Orlovskaya N.Compos Part Eng, 2004; 35B: 167 | | [14] | Chu C, Wang J, Lee S.Int J Hydrogen Energy, 2008; 33: 2536 | | [15] | Yang Z, Xia G, Maupin G D, Stevenson J W.J Electrochem Soc, 2006; 153: A1852 | | [16] | Shaigan N, Ivey D G, Chen W.J Power Sources, 2008; 183: 651 | | [17] | Qu W, Jian L, Hill J W, Ivey D G.J Power Sources, 2006; 153: 114 | | [18] | Wei W, Chen W, Ivey D G.J Power Sources, 2009; 186: 428 | | [19] | Hua B, Pu J, Gong W, Zhang J F, Lu F S, Jian L.J Power Sources, 2008; 185: 419 | | [20] | Bateni M R, Wei P, Deng X, Petric A.Surf Coat Technol, 2007; 201: 4677 | | [21] | Hua B, Zhang J F, Lu F S, Kong Y H, Pu J, Li J.Acta Metall Sin, 2009; 45: 605 | | [21] | (华斌, 张建福, 卢凤双, 孔永红, 蒲健, 李箭. 金属学报, 2009; 45: 605) | | [22] | Shannon R D. Acta Cryst, 1976; 32A: 751 | | [23] | Li J, Pu J, Hua B, Xie G Y.J Power Sources, 2006; 159: 641 | | [24] | Quadakkers W J, Piron-Abellan J, Shemet V.Mater High Temp, 2003; 20: 115 |
|
|