| 基于金属磁记忆评价裂纹埋深对激光熔覆层应力的影响* |
刘彬1,贡凯1,乔岩欣1( ),董世运2 |
1 江苏科技大学江苏省先进焊接技术重点实验室, 镇江 212003 2 装甲兵工程学院再制造技术重点实验室, 北京 100072 |
|
| EVALUATION OF INFLUENCE OF PRESET CRACK BURIAL DEPTH ON STRESS OF LASER CLADDING COATING WITH METAL MAGNETIC MEMORY |
Bin LIU1,Kai GONG1,Yanxin QIAO1( ),Shiyun DONG2 |
1 Key Laboratory of Advanced Welding Technology of Jiangsu Province, Jiangsu University of Science and Technology, Zhenjiang 212003, China 2 National Key Laboratory for Remanufacturing, Academy of Armored Forces Engineering, Beijing 100072, China |
引用本文:
刘彬,贡凯,乔岩欣,董世运. 基于金属磁记忆评价裂纹埋深对激光熔覆层应力的影响*[J]. 金属学报, 2016, 52(2): 241-248.
Bin LIU,
Kai GONG,
Yanxin QIAO,
Shiyun DONG.
EVALUATION OF INFLUENCE OF PRESET CRACK BURIAL DEPTH ON STRESS OF LASER CLADDING COATING WITH METAL MAGNETIC MEMORY[J]. Acta Metall Sin, 2016, 52(2): 241-248.
| [1] | Xu F.PhD Dissertation, Zhejiang University, Hangzhou, 2013 | | [1] | (徐帆. 浙江大学博士学位论文, 杭州, 2013) | | [2] | Tomohiro Y, Shinji Y, Masahiko H.NDT&E Int, 1996; 29: 263 | | [3] | Dovbov A A.Therm Eng, 2001; 48: 289 | | [4] | Zhang W M, Dong S P, Zhang Z J.Chin Mech Eng, 2003; 14: 892 | | [4] | (张卫民, 董韶平, 张之敬. 中国机械工程, 2003; 14: 892) | | [5] | Liu D X. Master Thesis, Yanshan University, Qinhuangdao, 2010 | | [5] | (刘东旭. 燕山大学硕士学位论文, 秦皇岛, 2010) | | [6] | Wang Z D, Yao K, Deng B, Ding K Q.NDT&E Int, 2010; 43: 513 | | [7] | Iordache V E, Hug E, Buiron N.Mater Sci Eng, 2003; A359: 62 | | [8] | Doubov A A.NDT&E Int, 2000; 33: 351 | | [9] | Pearson J, Squire P T, Maylin M G, Gore J G.IEEE Trans Magn, 2000; 36: 3251 | | [10] | Huang S L, Li L M, Shi K R, Wang X F.J Centr South Univ Technol, 2004; 11: 23 | | [11] | Dai G, Wang W J, Li W.Nondestruct Test, 2002; 24: 262 | | [11] | (戴光, 王文江, 李伟. 无损检测, 2002; 24: 262) | | [12] | Shi C L. PhD Dissertation, Harbin Institute of Technology, 2011 | | [12] | (石常亮. 哈尔滨工业大学博士学位论文, 2011) | | [13] | Xu B S, Dong L H, Dong S Y, Xue N.Acta Metall Sin, 2011; 47: 257 | | [13] | (徐滨士, 董丽虹, 董世运, 薛楠. 金属学报, 2011; 47: 257) | | [14] | Leng J C, Liu Y, Zhou G Q, Gao Y T.NDT&E Int, 2013; 55: 42 | | [15] | Dong L H, Xu B S, Dong S Y, Li S, Chen Q Z, Wang D.NDT&E Int, 2009; 42: 323 | | [16] | Shi C L, Dong S Y, Xu B S, He P.J Magn Magn Mater, 2010; 322: 413 | | [17] | Qin Y J, Wu Y P, Zhang J F, Guo W M, Hong S, Chen L Y.Trans Nonferrous Met Soc China, 2015; 25: 1144 | | [18] | Shan L, Wang X Y, Li J L, Li H, Lu X, Chen J M.Trans Nonferrous Met Soc China, 2015; 25: 1135 | | [19] | Lu Z, Kim M S, Myoung S W, Lee J H, Jung Y G, Kin I S, Jo C Y.Trans Nonferrous Met Soc China, 2014; 24(S1): 29 | | [20] | Wang Q Y, Bai S L, Liu Z D.Trans Nonferrous Met Soc China, 2014; 24: 1610 | | [21] | He X L, Wei Y H, Hou L F, Yan Z F, Guo C L, Han P J.Trans Nonferrous Met Soc China, 2014; 24: 3429 | | [22] | Ariely S.Surf Coat Technol, 1991; 45: 403 | | [23] | Lin Y H, Lei Y P, Fu H G, Lin J.Acta Metall Sin, 2014; 50: 1513 | | [23] | (林英华, 雷永平, 符寒光, 林健. 金属学报, 2014; 50: 1513) | | [24] | Feng S R, Tang H B, Zhang S Q, Wang H M.Trans Nonferrous Met Soc China, 2012; 22: 1667 | | [25] | Liu B, Chen S J, Dong S Y, Fang C F, Hu Q X, Guo Y.Trans China Weld Inst, 2015; 36(8): 23 | | [25] | (刘彬, 陈书锦, 董世运, 方臣富, 胡庆贤, 郭宇. 焊接学报, 2015; 36(8): 23) | | [26] | American Society for Nondestructive Testing, translated by Society for Nondestructive Testing. Nondestructive Testing Handbook-Electromagnetic Roll. Beijing: World Book Publising, 1994: 166 | | [26] | (美国无损检测学会编, 无损检测学会译. 无损检测手册-电磁卷. 北京: 世界图书出版社, 1994: 166) | | [27] | Wang H P, Dong S Y, Dong L H, Xu B S.Mater Eng, 2010; (12): 35 | | [27] | (王慧鹏, 董世运, 董丽虹, 徐滨士. 材料工程, 2010; (12): 35) | | [28] | Zhang W M, Liu H G, Yuan J J, Sun H T.Trans Beijing Inst Technol, 2005; 25: 1003 | | [28] | (张卫民, 刘红光, 袁俊杰, 孙海涛. 北京理工大学学报, 2005; 25: 1003 |
|
|