| 超临界CO2/油/水系统中油气管材钢的腐蚀机制* |
孙冲1, 孙建波1( ), 王勇1, 王世杰2, 刘建新2 |
1 中国石油大学(华东)机电工程学院, 青岛 266580 2 中石化胜利油田分公司采油工艺研究院, 东营 257000 |
|
| CORROSION MECHANISM OF OCTG CARBON STEEL IN SUPERCRITICAL CO2/OIL/WATER SYSTEM |
SUN Chong1, SUN Jianbo1( ), WANG Yong1, WANG Shijie2, LIU Jianxin2 |
1 College of Mechanical and Electronic Engineering, China University of Petroleum, Qingdao 266580 2 Oil Production Research Institute, Shengli Oilfield of Sinopec, Dongying 257000 |
引用本文:
孙冲, 孙建波, 王勇, 王世杰, 刘建新. 超临界CO2/油/水系统中油气管材钢的腐蚀机制*[J]. 金属学报, 2014, 50(7): 811-820.
Chong SUN,
Jianbo SUN,
Yong WANG,
Shijie WANG,
Jianxin LIU.
CORROSION MECHANISM OF OCTG CARBON STEEL IN SUPERCRITICAL CO2/OIL/WATER SYSTEM[J]. Acta Metall Sin, 2014, 50(7): 811-820.
| [1] |
Kermani M B, Morshed A. Corrosion, 2003; 59: 659
|
| [2] |
Zhang X Y,Di C,Lei L C. Corrosion and Control of CO2. Beijing: Chemical Industry Press, 2000: 15
|
| [2] |
(张学元,邸 超,雷良才. 二氧化碳腐蚀与控制. 北京: 化学工业出版社, 2000: 15)
|
| [3] |
Efird K D, Jasinski R J. Corrosion, 1989; 45: 165
|
| [4] |
Castillo M, Rincón H, Duplat S, Vera J, Bacón E. Corrosion 2000, Houston: NACE, 2000: 00005
|
| [5] |
Méndez C, Duplat S, Hernández S, Vera J. Corrosion 2001, Houston: NACE, 2001: 01030
|
| [6] |
De Waard C, Smith L M, Craig B D. Corrosion 2003, Houston: NACE, 2003: 03629
|
| [7] |
Efird K D, Smith J L, Blevins S E, Davis N D. Corrosion 2004, Houston: NACE, 2004: 04366
|
| [8] |
Craig B D. Mater Perform, 1996; 8: 61
|
| [9] |
Hernandez S E, Duplat S, Vera J R, Baron E. Corrosion 2002, Houston: NACE, 2002: 02293
|
| [10] |
Ayello F, Robbins W, Richter S, Nesic S. Corrosion 2011, Houston: NACE, 2011: 11060
|
| [11] |
Wei A J, Huo F Y, Wang Q, Dang L, Huang J Z. Corros Prot, 2009; 30: 383
|
| [11] |
(魏爱军, 霍富永, 王 茜, 党 丽, 黄建忠. 腐蚀与防护, 2009; 30: 383)
|
| [12] |
Rincon H, Hernandez S, Salazar J, Case R, Vera J. Corrosion 99, Houston: NACE, 1999: 602
|
| [13] |
Wu S L, Cui Z D, Li C F, Zhu S L, Yang X J. J Chin Soc Corros Prot, 2003; 23: 340
|
| [13] |
(吴水林, 崔振铎, 李春富, 朱胜利, 杨贤金. 中国腐蚀与防护学报, 2003; 23: 340)
|
| [14] |
Cui Z D, Wu S L, Zhu S L, Yang X J. Appl Surf Sci, 2006; 252: 2368
|
| [15] |
Sun J B, Liu W, Chang W, Zhang Z H, Li Z T, Yu T, Lu M X. Acta Metall Sin, 2009; 45: 84
|
| [15] |
(孙建波, 柳 伟, 常 炜, 张忠铧, 李忠涛, 于 湉, 路民旭. 金属学报, 2009; 45: 84)
|
| [16] |
Cui Z D, Wu S L, Li C F, Zhu S L, Yang X J. Mater Lett, 2004; 58: 1035
|
| [17] |
King M B, Mubarak A, Kim J D. J Supercrit Fluids, 1992; 5: 296
|
| [18] |
Choi Y S, Nesic S. Corrosion 2009, Houston: NACE, 2009: 09256
|
| [19] |
Zhang Y C, Gao K W, Schmitt G. Corrosion 2011, Houston: NACE, 2011: 11378
|
| [20] |
Dugstad A. Corrosion 2006, Houston: NACE, 2006: 06111
|
| [21] |
Chen C F, Lu M X, Zhao G X, Bai Z Q, Yan M L, Yang Y Q. Acta Metall Sin, 2002; 38: 411
|
| [21] |
(陈长风, 路民旭, 赵国仙, 白真权, 严密林, 杨延清. 金属学报, 2002; 38: 411)
|
| [22] |
Sun J B, Zhang G A, Liu W, Lu M X. Corros Sci, 2012; 57: 131
|
| [23] |
Cheng C F, Zhao G X, Lu M X, Yang Y Q, Li H L. J Chin Soc Corros Prot, 2002; 22: 143
|
| [23] |
(陈长风, 赵国仙, 路民旭, 杨延清, 李鹤林. 中国腐蚀与防护学报, 2002; 22: 143)
|
| [24] |
Lotz U, Van Bodegom L, Ouwehand C. Corrosion, 1991; 47: 635
|
| [25] |
Zhao G X. Physical Chemistry of Surfactant. Beijing: Peking University Press, 1984: 387
|
| [25] |
(赵国玺. 表面活性剂物理化学. 北京: 北京大学出版社, 1984: 387)
|
| [26] |
Carew J A, Al-Sayegh A, Al-Hashem A. Corrosion 2000, Houston: NACE, 2000: 00061
|
| [27] |
Nesic S. Corros Sci, 2007; 49: 4308
|
| [28] |
Chen C F, Lu M X, Chang W, Zhao G X, Bai Z Q. Corrosion 2003, Houston: NACE, 2003: 03342
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|