Please wait a minute...
金属学报  2013, Vol. 49 Issue (9): 1143-1147    DOI: 10.3724/SP.J.1037.2013.00179
  论文 本期目录 | 过刊浏览 |
三元β-Ti-Mo-Zr(Sn)合金析出相对弹性模量和力学性能的影响
李群,王清,李晓娜,高晓霞,董闯
大连理工大学三束材料改性教育部重点实验室, 大连理工大学材料科学与工程学院, 大连 116024
INFLUENCES OF PHASE PRECIPITATIONS OF TERNARY β-Ti-Mo-Zr(Sn) ALLOYS ON YOUNG'S MODULUS AND MECHANICAL PROPERTIES
LI Qun, WANG Qing, LI Xiaona, GAO Xiaoxia, DONG Chuang
Key Laboratory of Materials Modification by Laser, Ion and Electron Beams, Ministry of Education,School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024
引用本文:

李群,王清,李晓娜,高晓霞,董闯. 三元β-Ti-Mo-Zr(Sn)合金析出相对弹性模量和力学性能的影响[J]. 金属学报, 2013, 49(9): 1143-1147.
LI Qun, WANG Qing, LI Xiaona, GAO Xiaoxia, DONG Chuang. INFLUENCES OF PHASE PRECIPITATIONS OF TERNARY β-Ti-Mo-Zr(Sn) ALLOYS ON YOUNG'S MODULUS AND MECHANICAL PROPERTIES[J]. Acta Metall Sin, 2013, 49(9): 1143-1147.

全文: PDF(2606 KB)  
摘要: 

研究了低弹性模量β-Ti合金[MoTi14]Zr1(Ti78.2Mo11.2Zr10.6)和[SnTi14]Mo1(Ti75.7Mo10.9Sn13.4)中第二相析出对弹性模量和力学性能的影响及其拉伸过程中合金组成相的变化.利用Cu模吸铸快冷技术制备了直径6 mm的合金棒,并采用XRD和TEM分析合金拉伸前后的相析出行为及组织. 结果表明,在β基体上只有少量α〞的析出使得[SnTi14]Mo1合金具有较低的弹性模量(70 GPa),而ω相的存在使得[MoTi14]Zr1合金的弹性模量略高(80 GPa);且[SnTi14]Mo1合金中较细的薄片状β孪晶组织使得合金具有优良的力学性能.在拉伸过程中, [MoTi14]Zr1合金中应力诱发的马氏体含量增加,而在[SnTi14]Mo1合金中β基体晶粒易于发生扭转, 从而合金塑性提高.

关键词 : Ti-Mo-Zr(Sn)合金,  β-Ti合金,  低弹性模量,  相析出    
Abstract:

The influences of second phase precipitations of low Young's modulus (E) β-Ti alloys [MoTi14]Zr1 (Ti78.2Mo11.2Zr10.6) and [SnTi14]Mo1(Ti75.7Mo10.9Sn13.4) on mechanical properties as well as the variation of phase constitutions of alloys during tensile test were investigated. Alloy rods with 6 mm diameter were prepared by copper-mould suction-cast method. Phase precipitations and microstructures of alloys before and after tension were analyzed by XRD and TEM techniques. The experimental results showed that only a minor amount of   α〞martensite precipitated on β matrix makes the suction-cast [SnTi14]Mo1 alloy possess lower E with a value of 70 GPa, while ω precipitation increases the E (80 GPa) of [MoTi14]Zr1 alloy. It is due to the thinner β plate twins that makes [SnTi14]Mo1 alloy have better mechanical properties. During tensile testing, the amount of  α〞martensite induced by stress increases in [MoTi14]Zr1 alloy while β grains in [SnTi14]Mo1 alloy are easier to be rotated for deformation, which favors to enhance the ductility of alloys.

Key words: Ti-Mo-Zr(Sn) alloy    β-Ti alloy    low Young's modulus    phase precipitation
收稿日期: 2013-03-31     
基金资助:

国家自然科学基金项目51171035, 11174044和51131002资助

作者简介: 李群, 女, 1989年生, 硕士生

[1] Long M, Rack H J.  Biomaterials, 1998; 19: 1621

[2] Niinomi M.  Mater Sci Eng, 1998; A243: 231
[3] Saito T, Furuta T, Hwang J-H, Kuramoto S, Nishino K, Suzuki N, Chen R,Yamada A, Ito K, Seno Y.  Science, 2003; 300: 464
[4] Ahmed T, Long M, Silvestri J, Ruiz C, Rack H J. In: Blenkinsop P, Evans W J, Flower H M eds.,  Preceeding 8th World Titanium Conference, Birmingham, UK: The Institute of Metals, 1996: 1760
[5] Ikeda M, Komatsu S-Y, Sowa I, Niinomi M.  Metall Mater Trans, 2002; 33A: 487
[6] Hao Y L, Li S J, Sun S Y, Zheng C Y, Yang R.  Acta Biomater, 2007; 3: 277
[7] Ho W-F.  J Med Biol Eng, 2008; 28(1): 47
[8] Guo S, Bao Z Z, Meng Q K, Hu L, Zhao X Q.  Metall Mater Trans, 2012; 43A: 3447
[9] Abdel-Hady M, Hinoshita K, Morinaga M.  Scr Mater, 2006; 55: 477
[10] Hao Y L, Yang R, Niinomi M, Kuroda D, Zhou Y L, Fukunaga K, Suzuki A.Metall Mater Trans, 2002; 33A: 3137
[11] Wood R M.  Acta Metall, 1963; 11: 907
[12] Talling R J, Dashwood R J, Jackson M, Dye D.  Acta Mater, 2009; 57: 1188
[13] Zhao X L, Niinomi M, Nakai M, Miyamoto G, Furuhara T.  Acta Biomater, 2011; 7: 3230
[14] Dong C, Wang Q, Qiang J B, Wang Y M, Jiang N, Han G, Li Y H, Wu J, Xia J H.  J Phys, 2007; 40D: R273
[15] Hao C P, Wang Q, Ma R T, Wang Y M, Qiang J B, Dong C.  Acta Phys Sin, 2011; 60: 116101
(郝传璞, 王清, 马仁涛, 王英敏, 羌建兵, 董闯. 物理学报, 2011; 60: 116101)
[16] Wang Q, Ji C J, Wang Y M, Qiang J B, Dong C.  Metall Mater Trans, 2013; 44A: 1872
[17] Ma R T, Hao C P, Wang Q, Ren M F, Wang Y M, Dong C.  Acta Metall Sin, 2010; 46: 1034
(马仁涛, 郝传璞, 王清, 任明法, 王英敏, 董闯. 金属学报, 2010; 46: 1034)
[18] Takeuchi A, Inoue A.  Mater Trans, 2005; 46: 2817
[19] Hao Y L, Li S J, Sun S Y, Yang R.  Mater Sci Eng, 2006; A441: 112
[20] Moffat D L, Larbalestier D C.  Metall Mater Trans, 1988; 19A: 1677
[21] Xu Z Y.  Acta Metall Sin, 1997; 33: 45
(徐祖耀. 金属学报, 1997; 33: 45)
[22] Huang L J.  PhD Dissertation, Beijing Institute of Aeronautical Material, 2006
(黄利军. 北京航空材料研究院博士学位论文, 2006)
[23] Niinomi M.  Mater Sci Eng, 1998; A243: 231
[24] Martins D Q, Osorio W R, Souza M E, Caram R, Garcia A.  Electrochim Acta, 2008; 53: 2809
[25] Bania P J.  J Met, 1994; 64(7): 16
[1] 林晓冬,彭群家,韩恩厚,柯伟. 退火对热老化308L不锈钢焊材显微结构的影响[J]. 金属学报, 2019, 55(5): 555-565.
[2] 马仁涛 郝传璞 王清 任明法 王英敏 董闯. 低弹bcc结构Ti-Mo-Nb-Zr固溶体合金的“团簇+连接原子”模型及其成分设计[J]. 金属学报, 2010, 46(9): 1034-1040.
[3] 由园; 闫牧夫; 陈义强 . 低体积分数相析出过程的相场模拟[J]. 金属学报, 2008, 44(10): 1171-1174 .
[4] 李应举; 杨院生; 冯小辉; 张宇男; 胡壮麒 . 直流电流对一种镍基单晶高温合金 γ '相析出的影响[J]. 金属学报, 2006, 42(9): 942-946 .
[5] 杨锐;李东;万晓景. Ti-Al-La三元系中α_2相析出相界[J]. 金属学报, 1988, 24(4): 288-290.