|
|
|
| Gasar连铸工艺制备藕状多孔Cu-Zn合金 |
| 李再久,金青林,杨天武,蒋业华,周荣 |
| 昆明理工大学材料科学与工程学院,昆明650093 |
|
| FABRICATION OF LOTUS-TYPE POROUS Cu-Zn ALLOYS WITH THE GASAR CONTINUOUS CASTING PROCESS |
| LI Zaijiu, JIN Qinglin, YANG Tianwu, JIANG Yehua, ZHOU Rong |
| Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093 |
引用本文:
李再久,金青林,杨天武,蒋业华,周荣. Gasar连铸工艺制备藕状多孔Cu-Zn合金[J]. 金属学报, 2013, 49(6): 757-762.
LI Zaijiu,
JIN Qinglin,
YANG Tianwu,
JIANG Yehua,
ZHOU Rong.
FABRICATION OF LOTUS-TYPE POROUS Cu-Zn ALLOYS WITH THE GASAR CONTINUOUS CASTING PROCESS[J]. Acta Metall Sin, 2013, 49(6): 757-762.
| [1]Shapovalov V I. US Pat, 5181549, 1993
[2]Liu Y, Li Y X, Zhang H W. Acta Metall Sin, 2004;40: 1121
(刘源, 李言祥, 张华伟. 金属学报, 2004; 40: 1121)
[3]Yamamura S, Shiota H, Murakami K, Nakajima H. Mater Sci Eng, 2001; A318: 137
[4]Xie J X, Liu X H, Liu X F, Fang Y C, Wang H. Chin J Nonferrous Met, 2005; 15: 1869
(谢建新, 刘新华, 刘雪峰, 方玉诚, 王浩. 中国有色金属学报,2005; 15: 1869)
[5]Liu P S. Introduction to Cellular Materials.Beijing: Tsinghua University Press, 1999: 6
(刘培生. 多孔材料引论. 北京: 清华大学出版社, 1999: 6)
[6]Park J S, Hyun S K, Suzuki S, Nakajima H. Acta Mater, 2007; 55: 5646
[7]Jiang G R. PhD Dissertation, Tsinghua University,Beijing, 2010
(蒋光锐. 清华大学博士学位论文, 北京, 2010)
[8]Nakajima H, Hyun S K, Ohashi K, Ota K, Murakami K.Colloids Surf, 2001; 179A: 209
[9]Hyun S K, Nakajima H. Mater Lett, 2003; 57: 3149
[10]Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2006;42: 1165
(张华伟, 李言祥, 刘源. 金属学报, 2006; 42: 1165)
[11]Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2007;43: 589
(张华伟, 李言祥, 刘源. 金属学报, 2007; 43: 589)
[12]Jiang G R, Li Y X, Liu Y. Trans Nonferrous Met Soc China, 2011; 21: 88
[13]Nakajima H. Prog Mater Sci, 2007; 52: 1091
[14]Liu Y, Li Y X, Liu R F, Zhou R, Jiang Y H, Li Z H.Acta Metall Sin, 2010; 46: 129
(刘源, 李言祥, 刘润发, 周荣, 蒋业华, 黎振华.金属学报, 2010; 46: 129)
[15]Park J S, Hyun S K, Suzuki S, Nakajima H. Metall Mater Trans, 2009; 40A: 406
[16]Suzuki S, Kim T B, Nakajima H. J Phys, 2009; 165:012068
[17]Zhang H W. PhD Dissertation, Tsinghua University,Beijing, 2006
(张华伟. 清华大学博士学位论文, 北京, 2006)
[18]Szekely J. Fluid Flow Phenomena in Metals Processing. Newyork: Academic Press, 1979: 323
[19]Iida T, Guthrie R. The Physical Properties of Liquid Metals. Oxford: Clarendon Press, 1988: 71, 183
[20]Zhang H W, Li Y X. Acta Phys Sin, 2007; 56: 4864
(张华伟, 李言祥. 物理学报, 2007; 56: 4864)
[21]Kashihara M, Yonetani H, Kobi T, Hyun S K, Suzuki S,Nakajima H. Mater Sci Eng, 2009; A524: 112
[22]Kujime T, Hyun S K, Nakajima H. Metall Mater Trans, 2006; 37A: 393
[23]Ikeda T, Aoki T, Nakajima H. Metall Mater Trans,2005; 36A: 77
[24]Murakami K, Nakajima H. Mater Trans, 2002; 43:2582
[25]Cui Z Q. Metallography and Heat Treatment.Beijing: China Machine Press, 2000: 429
(崔忠圻. 金属学与热处理. 北京:机械工业出版社, 2000: 429) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|