Please wait a minute...
金属学报  2013, Vol. 49 Issue (5): 513-522    DOI: 10.3724/SP.J.1037.2012.00760
  论文 本期目录 | 过刊浏览 |
连铸结晶器内氩气/钢液两相非稳态湍流特性的大涡模拟研究
刘中秋1),李宝宽1),姜茂发1),张立2),徐国栋2)
1)东北大学材料与冶金学院, 沈阳 110819
2)宝山钢铁股份有限公司, 上海 201900
LARGE EDDY SIMULATION OF UNSTEADY ARGON/STEEL TWO PHASE TURBULENT FLOW IN A CONTINUOUS CASTING MOLD
LIU Zhongqiu1), LI Baokuan1), JIANG Maofa1), ZHANG Li2), XU Guodong2)
1)Department of Materials and Metallurgy, Northeastern University, Shenyang 110819
2)Baoshan Iron and Steel Limited Company, Shanghai 201900
引用本文:

刘中秋,李宝宽,姜茂发,张立,徐国栋. 连铸结晶器内氩气/钢液两相非稳态湍流特性的大涡模拟研究[J]. 金属学报, 2013, 49(5): 513-522.
LIU Zhongqiu1, LI Baokuan1, JIANG Maofa1, ZHANG Li2, XU Guodong2. LARGE EDDY SIMULATION OF UNSTEADY ARGON/STEEL TWO PHASE TURBULENT FLOW IN A CONTINUOUS CASTING MOLD[J]. Acta Metall Sin, 2013, 49(5): 513-522.

全文: PDF(7358 KB)  
摘要: 

提出了一种连铸结晶器内氩气/钢液两相非稳态湍流流动的大涡模拟模型, 采用非齐次Euler-Euler双流体模型描述氩气/钢液两相流运动方程, 采用大涡模拟模型对湍流黏性力进行求解. 利用板坯探伤缺陷检测结果间接地验证了氩气/钢液两相非稳态湍流运动特征, 利用水模型实验结果验证了两相的非对称流动特征. 结果表明, 氩气泡的行为将直接影响结晶器内钢液的流动行为. 气泡在结晶器内的运动行为主要受吹Ar量和钢流量的影响, 其平均直径随着吹Ar量的增大而增大, 随着钢流量的增大而减小. 结晶器内的不对称流场具有不稳定性, 偏流是绝对的, 对称是暂时的、偶然的, 偏流的周期性不明显. 结晶器二冷区弯曲段的弧形形状对结晶器内部流场的影响较大, 偏流发生在弯曲段附近.

关键词 : 连铸结晶器,  两相流,  大涡模拟,  Euler-Euler模型    
Abstract:

A large eddy simulation of unsteady argon/steel two phase flow in a continuous casting mold is presented in this work. The inhomogeneous Euler-Euler approach is used to describe the equations of motion of the two phase flow. Large eddy simulation model is used to solve the turbulent viscosity force. The drag force, lift force and virtual mass force are incorporated in the model. And this model has been validated with a water model experiment and the measurements of the ultrasonic flaw detection. The predicted unsteady two phase turbulent flow characteristics were validated, indirectly, by the measurements of ultrasonic flaw detection. The predicted asymmetric flow was validated by the water model experiment. The simulation results show that the distribution of the bubble diameter is seen to depend on the argon gas and molten steel flow rates. The mean bubble diameter decreases with increasing the molten steel flow rate, but increases with increasing the argon gas flow rate. The asymmetric flow inside the mold was not stationary; the time intervals for changeover appeared to be vary random. It can be concluded that the shape of the bending part of the secondary cooling zone of mold is important to the asymmetric flow. The asymmetric flow occurrs near the bending section.

Key words: continuous casting mold    two phase flow    large eddy simulation    Euler-Euler approach
收稿日期: 2012-12-21     
基金资助:

国家自然科学基金资助项目50934008

作者简介: 刘中秋, 男, 1986年生, 博士生

[1] Bai H, Thomas B G. Metall Mater Trans, 2001; 32B: 253


[2] Bai H, Thomas B G. Metall Mater Trans, 2001; 32B: 269

[3] Zhang L F, Yang S B, Cai K K, Li J Y, Wang X G, Thomas B G. Metall Mater Trans, 2007; 38B: 63

[4] Yoshida J, Iguchi M, Yokoya S.  Tetsu Hagane, 2001; 87: 529

(吉田进, 井口学, 横谷真一郎. 铁と钢, 2001; 87: 529)

[5] Bessho N, Yoda R, Yamasaki H. Iron Steelmaker, 1991; 18: 39

[6] Thomas B G, Huang X, Sussman R C. Metall Mater Trans, 1994; 25B: 527

[7] Sanchez-Perez R, Morales R D, Palafox-Ramos J, Diaz-Cruz M. Metall Mater Trans, 2004; 35B: 85

[8] Sanchez-Perez R, Morales R D. ISIJ Int, 2003; 43: 637

[9] Bai H, Thomas B G. Metall Mater Trans, 2001; 32B: 1143

[10] Lee G G, Thomas B G, Kim S H. Met Mater Int, 2010; 16: 501

[11] Kubo N, Ishii T, Kubota J. ISIJ Int, 2002; 42: 1251

[12] Li B K, Okane T, Umeda T. Metall Mater Trans, 2000; 31B: 1491

[13] Li B K, Okane T, Umeda T. Metall Mater Trans, 2001; 32B: 1053

[14] Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 619

(于海歧, 朱苗勇. 金属学报, 2008; 44: 619)

[15] Wang Y F, Zhang L F. Metall Mater Trans, 2011; 42B: 1319

[16] Liu Z Q, Qi F S, Li B K, Tsukihashi F. J Iron Steel Res Int, 2011; 18: 243

[17] Hershey D E, Thomas B G, Najjar F M. Int J Numer Methods Fluids, 1993; 17: 23

[18] Moser R D, Kim J, Mansour NN. Phys Fluids, 1999; 4: 943

[19] Yuan Q, Sivaramakrishnan S, Vanka S P, Thomas B G. Metall Mater Trans, 2004; 35B: 967

[20] Li B K, Liu Z Q, Qi F S, Wang F, Xu G D. Acta Metall Sin, 2012; 48: 23

(李宝宽, 刘中秋, 齐凤升, 王芳, 徐国栋. 金属学报, 2012; 48: 23)

[21] Yuan Q, Thomas B G, Vanka S P. Metall Mater Trans, 2004; 35B: 685

[22] Qian Z D, Wu Y L. Acta Metall Sin, 2004; 40: 88

(钱忠东, 吴玉林. 金属学报, 2004; 40: 88)

[23] Real C, Miranda R, Vilchis C, Barron M, Hoyos L, Gonzalez J. ISIJ Int, 2006; 46: 1183

[24] Deen N G, Solberg T, Hjertager B H. Chem Eng Sci, 2011; 56: 6341

[25] Dhotre M T, Niceno B, Smith B L. Chem Eng J, 2008; 136: 337

[26] Jakobsen H A, Sannaes B H, Grevskott S, Svendsen H F. Ind Eng Chem Res, 1997; 36: 4052

[27] Sato Y, Sekoguchi K. Int J Multiphase Flow, 1975; 2: 79

[28] Smagorinsky J. Mon Weather Rev, 1963; 91: 99

[29] Singh V, Dash S K, Sunitha J S, Ajmani S K, Das A K. ISIJ Int, 2006; 46: 210

[30] Gupta D, Lahiri A K. Metall Mater Trans, 1996; 27B: 757

[31] Miki Y, Takeuchi S. ISIJ Int, 2003; 43: 1548
[1] 刘中秋, 李宝宽, 肖丽俊, 干勇. 连铸结晶器内高温熔体多相流模型化研究进展[J]. 金属学报, 2022, 58(10): 1236-1252.
[2] 王富强, 刘伟, 王兆文. 铝电解槽中局部阴极电流增大对电解质-铝液两相流场的影响[J]. 金属学报, 2020, 56(7): 1047-1056.
[3] 王波,沈诗怡,阮琰炜,程淑勇,彭望君,张捷宇. 冶金过程中的气液两相流模拟[J]. 金属学报, 2020, 56(4): 619-632.
[4] 刘畅, 李树森, 张立峰. RH精炼过程中气液两相流动及混匀现象的模拟研究[J]. 金属学报, 2018, 54(2): 347-356.
[5] 陈芝会 王恩刚 张兴武 王元华 朱明伟 赫冀成. 行波磁场下吹Ar过程中结晶器内气泡行为的研究[J]. 金属学报, 2012, 48(8): 951-956.
[6] 李宝宽 刘中秋 齐凤升 王芳 徐国栋. 薄板坯连铸结晶器非稳态湍流大涡模拟研究[J]. 金属学报, 2012, 48(1): 23-32.
[7] 姚军 Michael Fairweather 李宁. 粒状腐蚀产物在管道中的沉积机理[J]. 金属学报, 2011, 47(7): 804-808.
[8] 方信贤 白允强 王章忠. J4不锈钢及化学镀Ni-P和Ni-Cu-P镀层在液-固两相流中的冲刷腐蚀行为[J]. 金属学报, 2010, 46(2): 239-244.
[9] 许秀杰 邓安元 王恩刚 张林涛 张兴武 张永杰 赫冀成. 电磁软接触连铸圆坯表面振痕演变机理[J]. 金属学报, 2009, 45(4): 464-469.
[10] 孟祥宁 朱苗勇. 高拉速板坯连铸结晶器液态渣消耗机理分析[J]. 金属学报, 2009, 45(4): 485-489.
[11] 李帅君 熊守美 Mei Li John Allison. 应用两相流模型模拟压铸充型过程的卷气现象[J]. 金属学报, 2009, 45(10): 1153-1158.
[12] 李海丽; 赵九洲; 李中原; 何杰 . 对流对偏晶合金液--液相变过程的影响[J]. 金属学报, 2008, 44(9): 1081-1084 .
[13] 孟祥宁; 朱苗勇 . 高拉速板坯连铸结晶器液体摩擦机理分析[J]. 金属学报, 2008, 44(10): 1193-1197 .
[14] 孟祥宁; 朱苗勇; 程乃良 . 高拉速下连铸坯振痕形成机理及振动参数优化[J]. 金属学报, 2007, 43(8): 839-846 .
[15] 孟祥宁; 朱苗勇; 刘旭东; 程乃良; 江中块 . 高拉速连铸结晶器非正弦振动因子研究[J]. 金属学报, 2007, 43(2): 205-210 .