| 304不锈钢在3.5\%NaCl溶液中的点蚀动力学及机理 |
| 杜楠, 田文明, 赵晴, 陈四兵 |
| 南昌航空大学轻合金加工科学与技术国防重点学科实验室, 南昌 330063 |
|
| PITTING CORROSION DYNAMICS AND MECHANISMS OF 304 STAINLESS STEEL IN 3.5%NaCl SOLUTION |
| DU Nan, TIAN Wenming, ZHAO Qing, CHEN Sibing |
| National Defence Key Discipline Laboratory of Light Alloy Processing Science and Technology Institute, Nanchang Hangkong University, Nanchang 330063 |
引用本文:
杜楠 田文明 赵晴 陈四兵. 304不锈钢在3.5\%NaCl溶液中的点蚀动力学及机理[J]. 金属学报, 2012, 48(7): 807-814.
,
,
,
.
PITTING CORROSION DYNAMICS AND MECHANISMS OF 304 STAINLESS STEEL IN 3.5%NaCl SOLUTION[J]. Acta Metall Sin, 2012, 48(7): 807-814.
| [1] Liao J X, Jiang Y M,WuWW, Zhong C, Li J. Acta Metall Sin, 2006; 42: 1187(廖家兴, 蒋益明, 吴玮巍, 钟澄, 李劲. 金属学报, 2006; 42: 1187)[2] Han D, Jiang Y M, Deng B, Zhang L H, Zhang W, Li J. Acta Metall Sin, 2009; 45: 919(韩冬, 蒋益明, 邓博, 张丽华, 张伟, 李 劲. 金属学报, 2009; 45: 919)[3] Dong C F, Luo H, Xiao K, Sun T, LiuQ, Li XG. J Wuhan Univ Technol–Mater Sci, 2011; 26: 641[4] Li H B, Jiang Z H, Yang Y, Cao Y, Zhang Z R. J Metall Mater, 2009; 16: 517[5] Li G M, Guo X P, Zheng J S. J Iron Steel Res, 2004; 11(4): 47[6] Hu L H, Du N, Wang M F, Zhao Q. J Chin Soc Corros Prot, 2007; 27: 233(胡丽华, 杜楠, 王梅丰, 赵晴. 中国腐蚀与防护学报, 2007; 27: 233)[7] Hong J F, Tan H, Chen L D, Li J, Li L, Jiang Y M. Acta Metall Sin, 2011; 47: 1445(洪巨峰, 谭华, 陈林豆, 李 劲, 李莉, 蒋益明. 金属学报, 2011; 47: 1445)[8] Tan Y J, Balley S, Kinsella B. Corros Sci, 1996; 38: 1681[9] Smulko J, Darouicki K. J Electroanal Chem, 2003; 545: 59[10] Wang M F, Du N, Li X G, Zhao Q, Liu G. Corros Prot, 2009; 30(1): 29(王梅丰, 杜楠, 李晓刚, 赵 晴, 刘 刚. 腐蚀与防护, 2009; 30(1): 29)[11] Wang M F, Li X G, Du N, Huang Y Z, Korsunsky A. Electrochem Commun, 2008; 10: 1000[12] Pan Y, Zhang S P, Zhou J L, Li X G, Xiao Y D. Equip Environ Eng, 2010; 7(4): 67(潘莹, 张三平, 周建龙, 李晓刚, 萧以德. 装备环境工程, 2010; 7(4): 67)[13] Lian C H, Gao Y. Chem Eng Mach, 1995; 22(2): 87(梁成浩, 高扬. 化工机械, 1995; 22(2): 87)[14] Ye T, Gao C Z. Mater Prot, 2007; 40(11): 78(叶涛, 高灿柱. 材料保护, 2007; 40(11): 78)[15] Liu G. Master Dissertation, Nanchang Hangkong Univ, 2008(刘刚. 南昌航空大学硕士学位论文, 2008)[16] Pujar M G, Anita T, Shaikh H, Dayul R K, Khatak H S. J Mater Eng Perform, 2007; 16: 494[17] Jong J K. Met Mater Int, 2011; 17: 777[18] Du N, Huang L, Xu S, Wang L Q. Failure Anal Prev, 2009; 4: 71(杜楠, 黄乐, 徐 珊, 王力强. 失效分析与预防, 2009; 4: 71)[19] Du N, Liu G, Zhao Q. Mater Sci, 2008; 2: 326[20] Jong J K. Met Mater Int, 2009; 15: 279[21] Girija S, Kamachi U, Mudali B R. Appl Electrochem, 2011; 41: 973[22] Yu Q B, Sun Y. Hot Work Technol, 2010; 39(2): 1(于庆波, 孙莹. 材料热处理技术, 2010; 39(2): 1)[23] Chen Y F, Rairdan R, Luo J L. Appl Electrochem, 1998; 28: 1371[24] Zhang J Q, Zhang Z. J Chin Soc Corros Prot, 2002; 22: 241(张鉴清, 张昭. 中国腐蚀与防护学报, 2002; 22: 241)[25] Zhang Z, Zhang J Q. Chin J Nonferrous Met, 2001; 11: 284(张昭, 张鉴清. 中国有色金属学报, 2001; 11: 284)[26] Li L, Li X G, Dong C f, Cheng Y F. Corros Eng Sci Tech, 2011; 46: 340[27] Sun D M, Jiang Y M, Tang Y, Xiang Q W, Zhong C, Liao J X, Li J. Electrochim Acta, 2009; 54: 1558[28] Frankel G S. J Electrochem Soc, 1998; 145: 2186 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|