| Si含量对电弧离子镀Ti-Al-Si-N薄膜组织结构和力学性能的影响 |
| 时婧1), 裴志亮1), 宫骏1), 孙超1), MUDERS C M2), 姜辛2) |
1) 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016
2) Institute of Materials Engineering, University of Siegen, Paul-Bonatz-Strasse 9-11, Siegen 57076, Germany |
|
| EFFECT OF Si CONTENT ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ti-Al-Si-N FILMS DEPOSITED BY CATHODIC VACUUM
ARC ION PLATING |
| SHI Jing1), PEI Zhiliang1),GONG Jun1), SUN Chao1), MUDERS C M2), JIANG Xin2) |
1) State Key Laboratory for Corrosion and Protection, Insititute of Metal Research, Chinese Academy of Sciences, Shenyang
2) Institute of Materials Engineering, University of Siegen, Paul-Bonatz-Strasse 9-11, Siegen 57076, Germany |
引用本文:
时婧 裴志亮 宫骏 孙超 MUDERS C M 姜辛. Si含量对电弧离子镀Ti-Al-Si-N薄膜组织结构和力学性能的影响[J]. 金属学报, 2012, 48(11): 1349-1356.
.
EFFECT OF Si CONTENT ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ti-Al-Si-N FILMS DEPOSITED BY CATHODIC VACUUM
ARC ION PLATING[J]. Acta Metall Sin, 2012, 48(11): 1349-1356.
| [1] Tam P L, Zhou Z F, Shum PW, Li K Y. Thin Solid Films, 2008; 516: 5725[2] Shi J, Kumar A, Zhang L, Jiang X, Pei Z L, Gong J, Sun C. Surf Coat Technol, 2012; 206: 2947[3] Franz R, Neidhardt J, Kaindl R, Sartory B, Tessadri R, Lechthaler M, Polcik P, Mitterer C. Surf Coat Technol, 2009; 203: 1101[4] Pfeiler M, Kutschej K, Penoy M, Michotte C, Mitterer C, Kathrein M. Int J Refract Met Hard Mater, 2009; 27: 502[5] Vaz F, Rebouta L, Goudeau P, Girardeau T, Pacaud J, Rivi´ere J P, Traverse A. Surf Coat Technol, 2001; 146: 274[6] Xie Z W, Wang L P, Wang X F, Huang L, Lu Y, Yan J C. Trans Nonferrous Met Soc China, 2011; 21: 476[7] Santana A E, Karimi A, Derflinger V H, Sch¨utze A. Surf Coat Technol, 2004; 177–178: 334[8] Zhu Y C, Fujita K, Iwamoto N, Nagasaka H, Kataoka T. Surf Coat Technol, 2002; 158–159: 664[9] Moser M, Mayrhofer P H. Scr Mater, 2007; 57: 357[10] MoserM,Mayrhofer P H, Clemens H. Intermetallics, 2008; 16: 1206[11] Moser M, Mayrhofer P H, Sz´ekely L, S´afr´an G, Barna P B. Surf Coat Technol, 2008; 203: 148[12] Kutschej K, Fateh N, Mayrhofer P H, Kathrein M, Polcik P, Mitterer C. Surf Coat Technol, 2005; 200: 113[13] Durand–Drouhin O, Santana A E, Karimi A, Derflinger V H, Sch¨utze A. Surf Coat Technol, 2003; 163: 260[14] Vepˇrek S, M¨annling H D, Karvankova P, Prochazka J. Surf Coat Technol, 2006; 200: 3876[15] Carvalho S, Vaz F, Rebouta L, Schneider D, Cavaleiro A, Alves E. Surf Coat Technol, 2001; 142–144: 110[16] Kim S K, Vinh P V, Kim J H, Ngoc T. Surf Coat Technol, 2005; 200: 1391[17] Park I W, Choi S R, Suh J H, Park C G, Kim K H. Thin Solid Films, 2004; 447–448: 443[18] Oliver W C, Pharr G M. J Mater Res, 1992; 7: 1564[19] Diserens M, Patscheider J, L´evy F. Surf Coat Technol, 1998; 108–109: 241[20] Carvalho S, Ribeiro E, Rebouta L, Vaz F, Alves E, Schneider D, Cavaleiro A. Surf Coat Technol, 2003; 174–175: 984[21] Fuentes G G, Almandoz E, Pierrugues R, Mart´?nez R, Rodr´?guez R J, Caro J, Vilaseca M. Surf Coat Technol, 2010; 205: 1368[22] Chang C L, Lee J W, Tseng M D. Thin Solid Films, 2009; 517: 5231[23] Briggs D, Seah M P. Practical Surface Analysis: Auger and X–Ray Photoelectron Spectroscopy. 2nd Ed., Chichester: John Wiley & Sons Ltd, 1990: 201[24] Wagner C D, RiggsWM, Davis L E, Moulder J F, Mullenberg G E. Handbook of X–Ray Photoelectron Spectroscopy. Eden Prairie: Perkin–Elmer Corporation, 1979: 34[25] Kim G S, Kim B S, Lee S Y, Hahn J H. Thin Solid Films, 2006; 506–507: 128[26] Petch N J, Hall E O. J Iron Steel Inst, 1953; 174: 25[27] Tsui T Y, Pharr G M, Oliver W C, Bhatia C S, White R L, Andres S, Anders A, Brown I G. In: Bogy D B, Donley M S, Drory M D, Field J E eds., Mater Res Soc Symp Proc 383, Cambridge: Cambridge University Press, 1995: 447[28] Musil J. Surf Coat Technol, 2000; 125: 322 |
|