| 氯化物熔盐体系共电沉积法制备Mg-Li-Gd合金的研究 |
| 魏树权1, 2), 张密林1, 韩伟1, 颜永得1, 张斌1, 3) |
1) 哈尔滨工程大学材料科学与化学工程学院, 教育部超轻材料与表面技术重点实验室, 哈尔滨 150001
2) 哈尔滨师范大学化学化工学院, 哈尔滨 150025
3) 黑龙江省科学院石油化学研究院, 哈尔滨 150040 |
|
| STUDY ON ELECTROCHEMICAL CODEPOSITION OF Mg-Li-Gd ALLOYS FROM CHLORIDE MELTS |
| WEI Shuquan1, 2), ZHANG Milin1, HAN Wei1), YAN Yongde1, ZHANG Bin1, 3) |
1) Key Laboratory of Superlight Materials and Surface Technology (Ministry of Education), College of Materials Science and Chemical Engineering, Harbin Engineering University, Harbin 150001
2) College of Chemistry & Chemical Engineering, Harbin Normal University, Harbin 150025
3) Institute of Petrochemistry, HLJ Academy of Sciences, Harbin 150040 |
引用本文:
魏树权 张密林 韩伟 颜永得 张斌. 氯化物熔盐体系共电沉积法制备Mg-Li-Gd合金的研究[J]. 金属学报, 2011, 47(2): 173-178.
,
,
,
,
.
STUDY ON ELECTROCHEMICAL CODEPOSITION OF Mg-Li-Gd ALLOYS FROM CHLORIDE MELTS[J]. Acta Metall Sin, 2011, 47(2): 173-178.
| [1] Crawford P, Barrosa R, Mendez J, Foyos J, Es–said O S. J Mater Process Technol, 1996; 56: 108[2] Watanable H, Tsutsui H. Int J Plast, 2001; 17: 387[3] Dong S L, Imai T, Lim SW, Kanetake N, Saito N.J Mater Sci, 2007; 42: 5296[4] Wang T, Zhang M L, Wu R Z. Mater Lett, 2008; 62: 1846[5] Chang T C, Wang J Y, Chu C L, Lee S. Mater Lett, 2006; 60: 3272[6] Xu G X. Rare Earth Elements (part II). Beijing: Metallurgical Industry Press, 1995: 462(徐光宪. 稀土(下). 北京: 冶金工业出版社, 1995: 462)[7] Tanno O, Ohuchi K, Matuzawa K. J Jpn Inst Light Met, 1992; 42: 3[8] Anyanwu I A, Kamado S, Kojima Y. Mater Trans, 2001; 42: 1212[9] Luo Alan A. Mater Sci Forum, 2003; 419–422(I): 57[10] Jin G Y, Du W B, Li J H, Wu Y F. J Chin Rare Earth Soc, 2007; 25: 610(靳广永, 杜文博, 李建辉, 吴玉峰. 中国稀土学报, 2007; 25: 610)[11] Zhang M L, Yan Y D, Han W, Xue Y, Jing X Y, Liu X L, Wang S S, Zhang X M. Electrochemistry, 2009; 77: 699[12] Yan Y D, Zhang M L, Xue Y, Han W, Cao D X, Wei S Q. Electrochim Acta, 2009; 54: 3387[13] Yan Y D, Zhang M L, Xue Y, Han W, Cao D X, He L Y. J Appl Electrochem, 2009; 39: 455[14] HanW, Chen Q, Ye K, Yan Y D, ZhangML. Acta Metall Sin (Engl Lett), 2010; 23: 129[15] Yan Y D, Zhang M L, Xue Y, Han W, Cao D X, Jing X Y, He L Y, Yuan Y. Phys Chem Chem Phys, 2009; 11: 6148[16] Du S L, Wu M H, Du F Y, Liu Y M. Chin Rare Earths, 1987; 2: 59(杜森林, 吴美煌, 杜富英, 刘英明. 稀土, 1987; 2: 59)[17] Chu Y L. Master Dissertation, Harbin Engineering University, 2009(褚衍龙. 哈尔滨工程大学硕士论文, 2009) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|