| 受控脉冲穿孔等离子弧焊小孔热滞后效应的研究 |
| 贾传宝1, 2, 武传松1, 高进强1 |
1.山东大学材料液固结构演变与加工教育部重点实验室, 济南 250061
2.山东省科学院海洋仪器仪表研究所, 青岛 266001 |
|
| STUDY ON THE THERMAL LAG EFFECT OF KEYHOLE IN CONTROLLED PULSE KEY–HOLING PLASMA ARC WELDING |
| JIA Chuanbao 1,2, WU Chuansong 1, GAO Jinqiang 1 |
1. Key Lab for Solid–Liquid Structure Evolution and Materials Processing (Ministry of Education), Shandong University,Jinan 250061
2. Institute of Oceangraphic Instrumentation, Shandong Academy of Science, Qingdao 266001 |
引用本文:
贾传宝 武传松 高进强. 受控脉冲穿孔等离子弧焊小孔热滞后效应的研究[J]. 金属学报, 2010, 46(8): 991-996.
.
STUDY ON THE THERMAL LAG EFFECT OF KEYHOLE IN CONTROLLED PULSE KEY–HOLING PLASMA ARC WELDING[J]. Acta Metall Sin, 2010, 46(8): 991-996.
|
[1] Zhang Y M and Zhang S B. Weld. J., 1999, 75(2): 53s
[2] Zhang Y M, Zhang S B. Weld. J., 1998, 77(6): 57
[3] Martikainen J K and Moisio T J I. Weld. J., 1993, 72(7): 329
[4] Vilkas E P. 1 Weld. J., 1991, 70(4): 49
[5] Irving B. Weld. J., 1997, 76(1): 34
[6] Irving B. Weld. J., 1992, 71(12): 49
[7] Nunes A C., Weld. J., 1984, 63(9): 27
[8] Keanini R G and Rubinsky B. Weld. J., 1990, 69(6): 41
[9] Dong C L, Wu L and Shao Y C. Chinese J. Mech. Eng., 2000, 11(5): 577
(董春林, 吴林, 邵亦陈. 中国机械工程, 2000, 11(5): 577)
[10] Chen Q, Sun Z G, Sun J W, Wang Y W. Trans. Nonferrous Metals Society of China, 2004, 14(1): 116
[11] Zhu Y F, Zhang H, Dong C L. et al. Areospace Manufacturing Technology, 2002, (2): 22
(朱轶峰, 张慧, 董春林等. 航天制造技术, 2002, (2): 22)
[12] Song D F, Hu S S, Han J, Zhu Y X. Trans. China Weld. Institution, 2006, 27(6): 45
(宋东风, 胡绳荪, 韩俭, 朱玉欣.焊接学报, 2006, 27(6): 45)
[13] Zhu Y F, Zhang H, Shao Y C, Dong C L. Plasma Processing Technology, 1999 Supplement issue: 53
(朱轶峰, 张慧, 邵亦陈, 董春林.等离子加工技术, 1999年增刊: 53)
[14] Jia C B, Wu C S, Zhang Y M. Trans. Nonferrous Met. Soc. China, 2009, 19:
[15] Jia C B, Wu C S, Zhang Y M. Chinese Journal of Mechanical Engineering, 2010, in press
|
|