| D+离子束辐照对Ti膜的影响 |
| 王博宇1), 向伟1), 谈效华1), 戴晶怡1), 程亮1), 秦秀波2) |
1) 中国工程物理研究院电子工程研究所, 绵阳 621900
2) 中国科学院高能物理研究所核分析技术重点实验室, 北京 100049 |
|
| EFFECT OF D+ BEAM IRRADIATION ON Ti FILM |
| WANG Boyu1), XIANG Wei1), TAN Xiaohua1), DAI Jingyi1), CHENG Liang1), QIN Xiubo2) |
1) Institute of Electronic Engineering, China Academy of Engineering Physics, Mianyang 621900
2) Key Laboratory of Nuclear Analysis Techniques, Institute of High Energy Physics, Chinese Academy of Sciences, Beijing 100049 |
引用本文:
王博宇 向伟 谈效华 戴晶怡 程亮 秦秀波. D+离子束辐照对Ti膜的影响[J]. 金属学报, 2010, 46(7): 810-813.
,
.
EFFECT OF D+ BEAM IRRADIATION ON Ti FILM[J]. Acta Metall Sin, 2010, 46(7): 810-813.
| [1] Reijonen J. Nucl Instrum Methods Phys Res Sect, 2007; 261B: 272
[2] Pauli M, Kehayias, Joseph J, Kehayias. Nucl Instrum Methods Phys Res Sect, 2007; 261B: 827
[3] Aleksandrov V D, Bogolubov E P, Bochkarev O V, Korytko L A, Nazarov V I, Polkanov Y G, Ryzhkov V I, Khasaev T O. Appl Radiat Isot, 2005; 63: 537
[4] Lunardon M, Nebbia G, Pesente S. Appl Radiat Isot, 2004; 61: 43
[5] Jarman S E, Pinchin J, Brushwood J M. J Radioanal Nucl Chem, 2007; 271: 47
[6] Solano I, Reichenbach B, Schwoebel P R, Chichester D L, Holland C E, Hertz K L, Brainard J P. Nucl Instrum Methods Phys Res Sect, 2008; 587A: 76
[7] Li F, Chen Y X,Wan X J,Wang Q J, Liu Y Y. Acta Metall Sin, 2006; 42: 143
(李芳, 陈业新, 万晓景, 王青江, 刘羽寅. 金属学报, 2006; 42: 143)
[8] Hughey B J. Nucl Instrum Methods Phys Res Sect, 1995; 95B: 393
[9] Yao Z E, Chen S W, Su T L. Nuclear Tech, 2004; 27: 787
(姚泽恩, 陈尚文, 苏桐龄. 核技术, 2004; 27: 787)
[10] Miao S M, Lei M K. Acta Metall Sin, 2004; 40: 1221
(苗收谋, 雷明凯. 金属学报, 2004; 40: 1221)
[11] Zhu X P, Lei M K, Ma T C. Nucl Instrum Methods Phys Res Sect, 2003; 211B: 827
[12] Yonts O C, Strehlow R A. J Appl Phys, 1962; 33: 2903
[13] Uedono A, Tanigawa S. Appl Phys Lett, 1988; 53: 25
[14] Ziegler J F, Biersack J, Littmark U. The Stopping and Range of Ions in Matter. New York: Pergamon Press, 1985: 1 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|