| 两种位向关系的描述方法的转换及其应用 |
| 孟杨;张文征 |
| 清华大学材料科学与工程系先进材料实验室; 北京 100084 |
|
| CONVERTION AND ITS APPLICATION OF TWO KINDS OF DISCRIPTIONS ON THE ORIENTATION RELATIONSHIP |
| MENG Yang; ZHANG Wenzheng |
| Key Laboratory for Advanced Materials of Ministry of Education; Department of Materials Science and Engineering; Tsinghua University; Beijing 100084 |
引用本文:
孟杨 张文征. 两种位向关系的描述方法的转换及其应用[J]. 金属学报, 2010, 46(6): 647-656.
,
.
CONVERTION AND ITS APPLICATION OF TWO KINDS OF DISCRIPTIONS ON THE ORIENTATION RELATIONSHIP[J]. Acta Metall Sin, 2010, 46(6): 647-656.
| [1] Kurdjumov G V, Sachs G. Zeitschrift f¨ur Physik, 1930; 64: 325
[2] Nishiyama Z. Sci Rep Tohoku Imp Univ Ser 23, 1934; 23: 638
[3] Wassermann G. Mitt K–Wilh–Inst Eisenforsch, 1935; 17:149
[4] Dautovich D P, Bowles J S. Acta Metall Mater, 1972; 20: 1137
[5] Kelly P M, Jostsons A, Blake R G. Acta Metall Mater, 1990; 38: 1075
[6] Qiu D, Zhang W Z. Acta Mater, 2007; 55: 6754
[7] Kitahara H, Ueji R, Ueda M, Tsuji N, Minamino Y. Mater Charact, 2005; 54: 378
[8] Nolze G, Geist V. Cryst Res Technol, 2004; 39: 343
[9] He Y, Godet S, Jons J J. J Appl Cryst, 2006; 39: 72
[10] Furuhara T, Kawata H, Morito S, Maki T. Mater Sci Eng, 2006; A431: 228
[11] Furuhara T, Kawata H, Morito S, Miyamoto G, Maki T. Metall Mater Trans, 2008; 39A: 1003
[12] Miyamoto G, Takayama N, Furuhara T. Scr Mater, 2009; 60: 1113
[13] Yang P. Electron Backscatter Diffraction and its Application. Beijing: Metallurgical Industry Press, 2007: 55
(杨平. 电子背散射衍射技术及其应用. 北京: 冶金工业出版社, 2007: 55)
[14] Nolze G. Cryst Res Technol, 2006; 41: 72
[15] Wayman C M. Introduction to the Crystallography of Martensitic Transformations. New York: Macmillan, 1964: 115
[16] Wu J, Zhang W Z. Acta Metall Sin, 2009; 45: 897
(吴静, 张文征. 金属学报, 2009; 45: 897)
[17] Schwartz A J, Kumar M, Adams B L. Electron Backscatter Diffraction in Materials Science. New York: Kluwer Academic, 2000: 34 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|