| 固体透氧膜法直接还原NiO-CeO2制备CeNi5合金 |
| 赵炳建1;2; 鲁雄刚1; 李重河1; 钟庆东1 |
1. 上海大学上海市现代冶金与材料制备重点实验室; 上海 200072
2. 河北钢铁集团唐山钢铁股份有限公司; 唐山 063016 |
|
DIRECT ELECTROCHEMICAL REDUCTION OF NiO–CeO2 POWDER FOR PREPARATION OF CeNi5 ALLOY BY SOLID–OXYGEN–ION
CONDUCTING MEMBRANE PROCESS |
| ZHAO Bingjian1;2; LU Xionggang 1; LI Chonghe1;ZHONG Qingdong1 |
1. Shanghai Key Laboratory of Modern Metallurgy and Materials Processing; Shanghai University; Shanghai 200072
2. Tangshan Iron and Steel Co.; Ltd; Hebei Iron and Steel Group; Tangshan 063016 |
引用本文:
赵炳建 鲁雄刚 李重河 钟庆东. 固体透氧膜法直接还原NiO-CeO2制备CeNi5合金[J]. 金属学报, 2009, 45(10): 1255-1260.
.
DIRECT ELECTROCHEMICAL REDUCTION OF NiO–CeO2 POWDER FOR PREPARATION OF CeNi5 ALLOY BY SOLID–OXYGEN–ION
CONDUCTING MEMBRANE PROCESS[J]. Acta Metall Sin, 2009, 45(10): 1255-1260.
| [1] Nakamura H, Nguyen–Manh D, Pettifor D G. J Alloys Compd, 1998; 281: 81
[2] Kisi X L, Suda S Z. Phys Chem, 1989; 164: 1235
[3] Wang C S, Mariza M R, Daniel A S. Int J Hydrogen Energy, 2006; 31: 603
[4] Tang R, Liu L Q, Liu Y N, Yu G, Zhu J W, Liu X D. Chin J Nonferrous Met, 2005; 15: 1057
(唐睿, 刘丽琴, 柳永宁, 于光, 朱杰武, 刘晓东. 中国有色金属学报, 2005; 15: 1057)
[5] Dischinger J, Schaller H J. J Alloys Compd, 2000; 312:201
[6] Chen G Z, Farthing T W. Nature, 2000; 407: 361
[7] Schwandt C, Fray D J. Electrochim Acta, 2005; 51: 66
[8] Dai L, Zhao B J, Wang L, Cui G H, Zhu L G, Li L N. J Funct Mater, 2008; 39: 453
(戴 磊, 赵炳建, 王 岭, 崔广华, 朱立光, 李丽娜. 功能材料, 2008; 39: 453)
[9] Hu X F, Xu Q. Acta Metall Sin, 2006; 42: 285
(胡小峰, 许茜. 金属学报, 2006; 42: 285)
[10] Deng L Q, Xu Q, Ma T, Li B, Zhai Y C. Acta Metall Sin, 2005; 41: 551
(邓丽琴, 许茜, 马涛, 李兵, 翟玉春. 金属学报, 2005; 41: 551)
[11] Zhao B J, Wang L, Dai L, Cui G H, Li Y H, Zhu L G. PowdeMetall Ind, 2008; 18: 23
(赵炳建, 王岭, 戴磊, 崔广华, 李跃华, 朱立光. 粉末冶金工业, 2008; 18: 23)
[12] Zhao B J, Wang L, Dai L, Cui G H, Zhou H Z, Kumar R V. J Alloys Compd, 2009; 468: 379
[13] Qiu G H, Wang D H, Jin X B, Chen G Z. Electrochim Acta, 2006; 51: 5785
[14] Cheng H W, Lu X G, Li Q, Liu J M, Ding W Z, Zhou G Z. Acta Metall Sin, 2006; 42: 500
(程红伟, 鲁雄刚, 李谦, 刘建民, 丁伟中, 周国治. 金属学报, 2006; 42: 500)
[15] He L, Lu X G, Chen C Y, Li Q, Li C H, Zhong Q D. Chin J Nonferrous Met, 2008; 18: 1336
(何理, 鲁雄刚, 陈朝轶, 李谦, 李重河, 钟庆东. 中国有色金属学报, 2008; 18: 1336)
[16] Chen C Y, Lu X G. Acta Metall Sin, 2008; 44: 145
(陈朝轶, 鲁雄刚. 金属学报, 2008; 44: 145)
[17] Chen C Y, Lu X G, Li Q, Liu J M, Cheng H W, Zhou G Z. J Mater Metall, 2007; 6: 204
(陈朝轶, 鲁雄刚, 李谦, 刘建民, 程红伟, 周国治. 材料与冶金学报, 2007; 6: 204)
[18] Krishnan A, Lu X G, Pal U B. Scand J Metall, 2005; 34: 293
[19] Krishnan A, Lu X G, Pal U B. Metall Mater Trans, 2005; 36B: 463
[20] Elena G, Chen G Z, Fray D J. Electrochim Acta, 2004; 49: 2195
[21] Chen G Z, Elena G, Fray D J. Metall Mater Trans, 2004; 35B: 223 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|