| 深过冷条件下Fe-Ni-P-B合金的纳米晶凝固组织与液相Spinodal分解 |
| 张长青;姚可夫 |
| 清华大学 |
|
| The nanocrystalline structures of Fe-Ni-P-B alloy solidified at large undercooling and the liquid Spinonal decomposition of alloy melt |
| ; |
| 清华大学 |
引用本文:
张长青; 姚可夫 . 深过冷条件下Fe-Ni-P-B合金的纳米晶凝固组织与液相Spinodal分解[J]. 金属学报, 2006, 42(8): 870-874 .
,
.
The nanocrystalline structures of Fe-Ni-P-B alloy solidified at large undercooling and the liquid Spinonal decomposition of alloy melt[J]. Acta Metall Sin, 2006, 42(8): 870-874 .
[1]Long Y,Zhang Z Y,Li S W.New Functional Magnetic Material and Applications.Beijing:China Machine Press,1997:130 (龙毅,张正义,李守卫.新功能磁性材料及其应用.北京:机械工业出版社,1997:130) [2]Kui H W,Greer A L,Turnbull D.Appl Phys Lett,1984;45:615 [3]Perepezko J H.Mater Sci Eng,1994;A179:52 [4]Herlach D M,Gao J,Holland-Moritz D,Volkmann T.Mater Sci Eng,2004;A375:9 [5]Norman A F,Greer A L.Mater Sci Forum,1995;179-180:707 [6]Hu H Q.Principles of Metal Solidification.2nd ed,Beijing:China Machine Press,2000:80 (胡汉起.金属凝固原理.第2版,北京:机械工业出版社,2000:80) [7]Shen T D,Schwartz R B.Acta Mater,2001;49:837 [8]Cahn J W.TMS AIME,1968;242:166 [9]Guo W H,Chua C F,Leung C C,Kui H W.J Mater Res,2000;15:1605 [10]Luborsky F E.Amorphous Metallic and Alloys.London:Butterworth & Co (Publishers) Ltd.,1983:153 [11]Perepezko J H.Mater Sci Eng,1997;A226-228:374 [12]Laxmanan V.Acta Metall,1985;33:1475 [13]Xu Z,Zhao L C.Principles of Metallic Solid Transformation.Beijing:Science Press,2004:169 (徐洲,赵连城.金属固态相变原理.北京:科学出版社,2004:169) [14]Lee K L,Kui H W.J Mater Res,1999;14:3653 [15]Hong S Y,Guo W H,Kui H W.J Mater Res,1999;14:3668 [16]Guo W H,Kui H W.Acta Mater,2000;48:2117 [17]Yuen C W,Lee K L,Kui H W.J Mater Res,1997;12:314 [18]Yuen C W,Kui H W.J Mater Res,1998;13:3034w |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|