| Fe--C--Si--B--P--Cr--Mo--Al块体非晶合金的制备与压缩性能 |
| 李宏祥; Seonghoon Yi; 张新房; 王晓东 |
| 韩国庆北大学校材料科学及冶金系纳米结构材料实验室;大邱 702--701 |
|
| Preparation and Compression Properties of Fe--C--Si--B--P--Cr--Mo--Al Bulk Metallic Glass |
| LI Hongxiang; YI Seonghoon; ZHANG Xinfang; WANG Xiaodong |
| Nanostructured Materials Laboratory;Department of materials science and Metallurgy;Kyungpook National University;1370 Sankyuk-dong; Buk-gu; Daegu; 702-701; Korea |
引用本文:
李宏祥; Seonghoon.Yi; 张新房; 王晓东 . Fe--C--Si--B--P--Cr--Mo--Al块体非晶合金的制备与压缩性能[J]. 金属学报, 2006, 42(7): 777-780 .
,
,
,
.
Preparation and Compression Properties of Fe--C--Si--B--P--Cr--Mo--Al Bulk Metallic Glass[J]. Acta Metall Sin, 2006, 42(7): 777-780 .
[1] Ponnambalam V,Joseph P S,Shiflet G J.J Mater Res,2004; 19: 3046 [2] Ponnambalan V, Joseph P S, Shiflet G J, Kepl V M,Taylor R,Petculescu G.Appl Phys Lett, 2003; 83: 1131 [3] Shen T D, Schwarz R B. Appl Phys Lett, 1999; 75: 45 [4] Chen F F, Tsin C S, Zhou S X. Mater Sci Eng, 2004; A 373: 158 [5] Pang S J, Zhang T,Asami K. Acta. Mater, 2002; 50: 489 [6] Ponnambalam V, Joseph P S. J Mater Res, 2004; 19: 1320 [7] Lu Z P, Liu C T, Thompson J R, Porter W D. Phys Rev Lett, 2004; 92: 245503 [8] Inoue A, Wang X M. Acta Mater, 2000; 48: 1383 [9] Lim H K, Yi S, Kim W T, Kim D H, Kim S H, Kim N J.Scr Mater, 2001; 44: 1635 [10] Yi S, Kim K B, Sohn H S. Mater Trans, 2005; 46: 2237 [11] Li H X, Yi S. Mater Sci Eng, 2006; in Press [12] Lu Z P, Goh T T, Li Y, Ng S C. Acta Mater, 1999; 47:2215 [13] Lu Z P, Liu C T. Acta Mater, 2002; 50: 3501 [14] Lin C Y, Chin T S, Chao C K, Wang W H. Mater Trans,2004; 45: 888 [15] Kissinger M E. J Anal Chem, 1957; 29: 1702. [16] Mitrovic N, Roth S, Eckert J. Appl Phys Lett, 2001; 78:2145. [17] Inoue A, Gook J S. Mater Trans, 1995; 36: 1282. [18] Inoue A, Eun P Rae. Mater Trans, 1996; 37: 1715. [19] Inoue A, Shen B, Chang C T. Acta Mater, 2004; 52: 4093 [20] Stoica M, Eckert J, Roth S, Schultz L, Wang W H.Intermetallics, 2005; 13: 764; |
|