| 时效对Al-Cu合金中锯齿形流动的影响 |
| 江慧丰;张青川;徐毅豪;伍小平 |
| 中国科技大学中国科学院材料力学行为和设计重点实验室 |
|
引用本文:
江慧丰; 张青川; 徐毅豪; 伍小平 . 时效对Al-Cu合金中锯齿形流动的影响[J]. 金属学报, 2006, 42(2): 139-142 .
[1] Portevin A, Le Chatelier F. Comp Rend Acad Sci Paris, 1923; 176: 507 [2] Bell J F. Encyclopedia of Physics, Mechanics of Solids I. Berlin: Springer-Verlag Press, 1973: 41, 649 [3] Cottrell A H. Dislocations and Plastic Flow in Crystals. London: Oxford University Press, 1953: 1 [4] Beukel A V. Phys Status Solidi, 1975; 30a: 197 [5] Mulford R A, Kocks U F. Acta Metall, 1979; 27: 1125 [6] McCormick P G. Acta Metall, 1972; 20: 351 [7] Tian B H, Li H X, Zhang Y G, Chen C Q. Acta Metall Sin, 1998; 34: 603 (田宝辉,李焕喜,张永刚,陈昌麒.金属学报,1998;34:603) [8] Jiang H F, Zhang Q C, Jiang Z Y, Wu X P. Acta Metall Sin, 2005; 41: 727 (江慧丰,张青川,蒋震宇,伍小平.金属学报,2005;41:727) [9] Chihab K, Estrin Y, Kubin L P. Scr Metall, 1987; 21: 203 [10] Jiang H F, Zhang Q C, Jiang Z Y, Chen Z J, Wu X P. Chin Phys Lett, 2005; 22(1): 99 (江慧丰,张青川,蒋震宇,陈忠家,伍小平.中国物理快报,2005,22(1):99) [11] Picu R C. Acta Mater, 2004; 52: 3447 [12] Zhang Q C, Toyooka S, Meng Z B. In: SPIE, ed., Proc SPIE Conf on Nondestructive Evaluation of Aging Materials and Composites III, California: SPIE Press, 1999; 3585: 389 [13] McCormick P G. Scr Metall, 1972; 6: 165 [14] Kubin L P, Estrin Y. Acta Metall Mater, 1990; 38: 697 [15] Pink E. Strength of Metals and Alloys (ICSMA, 8). Oxford: Pergamon Press, 1988: 1l |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|