| 高纯铝箔在异步轧制和再结晶过程中取向的演变 |
| 黄 涛 曲家惠 胡卓超 王 福 左 良 |
| 东北大学材料与冶金学院;沈阳110004; 沈阳师范大学物理科学与技术学院;沈阳110034 |
|
| EVOLUTION OF THE ORIENTATION OF CROSS SHEAR ROLLING HIGH PURITY ALUMINUM FOILS DURING DEFORMATION AND RECRYSTALLIZATION |
| HUANG Tao; QU Jiahui;HU Zhuochao; WANG Fu;ZUO Liang |
| School of Materials and Metallurgy; Northeastern University; Shenyang 110004; College of Physical Science and Technology; Shenyang Normal University; Shenyang 110034 |
引用本文:
黄涛; 曲家惠; 胡卓超; 王福; 左良 . 高纯铝箔在异步轧制和再结晶过程中取向的演变[J]. 金属学报, 2005, 41(9): 953-957 .
,
,
,
,
.
EVOLUTION OF THE ORIENTATION OF CROSS SHEAR ROLLING HIGH PURITY ALUMINUM FOILS DURING DEFORMATION AND RECRYSTALLIZATION[J]. Acta Metall Sin, 2005, 41(9): 953-957 .
[1] Montheillet F, Cohen M, Jonas J J. Acta Metall, 1984; 32: 2077 [2] Hjelen J, (?)rsund R, Nes E. Acta Metall Mater , 1991; 39: 1377 [3] Engler O, Moo Y H. Mater Sci Eng, 1999; 271: 371 [4] Lu A Q, Jiang Q W, Wang F, Zuo L, Liang Z D. Acta Metall Sin, 2002; 38: 974 (吕爱强,蒋奇武,王福,左良,梁志德,金属学报,2002; 38:974) [5] Lu A Q, Huang T, Wang F, Zuo L. Chin J Nonferrous Met, 2003; 13: 56 (吕爱强,黄涛,王福,左良.中国有色金属学报,2003; 13:56) [6] Sun Y H, Huang T, Jia N, Wang F, Zuo L. Heat Treat Met, 2004; 29: 35 (孙永辉,黄 涛,贾 楠,王 福,左 良.金属热处理, 2004;29:35) [7] Liang Z D, Xu J Z, Wang F. Three Dimensional Orientation Distribution Analysis of Textured Materials. Shenyang: Northeastern University Press, 1986: 108 (梁志德,徐家桢,王福.织构材料三维取向分析术——ODF 分析.沈阳:东北工学院出版社, 1986:108) [8] Xu Z J, Jiang Q W, Zhao X, Wang F, Liang Z D. Met Phys Exam Test, 2001; (6): 36 (徐忠杰,蒋奇武,赵骧,王福,梁志德.物理测试,2001; (6):36) [9] Duggan B J, Lee C S. Scr Metall Mater, 1992; 27: 1503 [11] Hutchinson B. Scr Metall Mater, 1992; 27: 1471 [12] Zhu Q. Iron Steel, 1980; 15: 1 (朱泉.钢铁,1980;15:1) [13] Liu G, Wang F, Qi K M, Liu G L, Liang Z D. Acta Metall Sin, 1997; 33: 365 (刘刚,王福,齐克敏,刘佳兰,梁志德.金属学报,1997; 33:365) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|