| 亚共晶Al--Si合金变质级别的定量金相分析 |
| 陈 祥 耿慧远 李言祥 |
| (清华大学先进成形制造重点实验室; 清华大学机械工程系; 北京 100084) |
|
引用本文:
陈祥; 耿慧远; 李言祥 . 亚共晶Al--Si合金变质级别的定量金相分析[J]. 金属学报, 2005, 41(8): 891-896 .
[1] Chen Y H, Yan M. Mater Eng, 2000; 8: 121 (陈延红,严 密.材料科学与工艺,2000;8:121) [2] Croseley P E, Mondolfo L F. AFS Trans, 1966; 74: 53 [3] Paray F, Gruzleski J E. AFS Trans, 1994; 115: 833 [4] Apelian D, Sigworth G K, Whaler K R. AFS Trans, 1984; 92: 297 [5] Argyropoulos S, Closset B, Oger H. AFS Trans, 1983; 27: 351 [6] Qin G Y. Quantitative Metallography. Chengdu: Sichuan Science and Technology Press, 1987: 1 (秦国友.定量金相.成都:四川科学技术出版社, 1987:1) [7] Geng H Y, Li Y X, Chen X, Wang X. Proc 2004 Annual Gonf Special Casting & Nonferrous Alloys, Wuhan: Editorial Office of Special Casting & Nonferrous Alloys, 2004: 11 (耿慧远,李言祥,陈祥,王雪.特种铸造及有色合金2004 年年会专刊,武汉;特种铸造及有色合金编辑部, 2004:11) [8] Apelian D, Sigworth G K, Whaler K R. AFS Trans, 1984; 161: 297 [9] Jiang H, Sokolowski J H. AFS Trans, 2000; 108: 505 [10] Djurdjevic M, Jiang H, Sokolowski J. Mater Charact, 2001; 46: 31 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|