| 用CA方法模拟过冷熔体中自由树枝晶的生长 |
| 陈 晋 朱鸣芳 孙国雄 |
| (东南大学材料科学与工程系; 南京 210018) |
|
引用本文:
陈晋; 朱鸣芳; 孙国雄 . 用CA方法模拟过冷熔体中自由树枝晶的生长[J]. 金属学报, 2005, 41(8): 799-803 .
[1] Juric D, Tryggvason G. J Comput Phys, 1996; 123: 127 [2] Udaykumar H S, Mao L. Int J Heat Mass Transfer, 2002; 45: 4793 [3] Udaykumar H S, Marella S, Krishnan S. Int J Heat Mass Transfer, 2003; 46: 2615 [4] Kobayashi R. Physica, 1993; 63D: 410 [5] Warren J A, Boettinger W J. Acta Metall Mater, 1992; 43: 689 [6] Karma A, Rappel W J. Phys Rev, 1996; 53E: R3017 [7] Liu B C, Jing T. Simulation and Quality Control of Foundry Engineering. Beijing: China Machine Press, 2001: 178 (柳百成,荆 涛.铸造工程的模拟仿真与质量控制北京:机 械工业出版社,2001:178) [8] Sasikumar R, Jacob E, George B. Scr Mater, 1998; 38: 693 [9] Dilthey U, Pavlik V. In: Thomas B G, Beckermann C, eds., Modeling of Casting, Welding and Advanced Solidification Processes VIII, Warrendale PA: TMS, 1998: 589 [10] Nastac L. Acta Mater, 1999; 47: 4253 [11] Beltran-Sanchez L, Stefanescu D M. Metall Mater Trans, 2003; 34A: 367 [12] Jacot A, Rappaz M. Acta Mater, 2002; 50: 1909 [13] Li Q, Li D Z, Qian B N. Acta Metall Sin, 2004; 40: 634 (李强,李殿中,钱百年.金属学报, 2004;40:634) [14] Xie S Y. Vector Analysis and Field Theory. Beijing: Higher Education Press, 1985: 27 (谢树艺.矢量分析与场论.北京:高等教育出版社,1985:27) [15] Rider W J, Kothey D B. J Comput Phys, 1998; 141: 112 [16] Min N B. Physical Fundamentals of Crystal Growth. Shanghai: Shanghai Science and Technology Press, 1982: 230 (闵乃本.晶体生长的物理基础.上海:上海科技出版社,1982: 230) [17] Lipton J, Glicksman M E, Kurz W. Mater Sci Eng, 1984; 65: 57 [18] Glicksman M E, Marsh S P. Handbook of Crystal Growth I, Part B. Amsterdam: North-Holland, 1993: 1078 [19] Zhu M F, Hong C P. ISIJ Int, 2001; 41: 436A |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|