| Ag-Ti二元系在980, 1100和1200℃下的相平衡测量 |
| 傅晓亮 李长荣 李 梅 张维敬 |
| 北京科技大学材料科学与工程学院; 北京 100083 |
|
| Determination of the Phase Equilibrium of the Ag-Ti Binary System at 980, 1100 and 1200℃ |
| FU Xiaoliang; LI Changrong; LI Mei; ZHANG Weijing |
| School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
傅晓亮; 李长荣; 李梅; 张维敬 . Ag-Ti二元系在980, 1100和1200℃下的相平衡测量[J]. 金属学报, 2005, 41(7): 691-694 .
,
,
,
.
Determination of the Phase Equilibrium of the Ag-Ti Binary System at 980, 1100 and 1200℃[J]. Acta Metall Sin, 2005, 41(7): 691-694 .
[1]Wallbaum H J.Naturwissenschaften,1943;31:91 [2]Raub E,Walter P,Engel M.Z MetaLLkd,1952;43:112 [3]van Thype R J,Rostoker W,Kessler H D.j Met,1953; 3:670 [4]Adenstedt H K,Freeman W.WADC Technol Rep,Part 1 1953:53 [5]McQuillan M K.J Inst Met,1960;88:235. [6]Eremenko V N,Buyanov Y I,Panchenko N M.Porosh Metall,1969;79:55 [7]Plichta M R,Aaronson H I.Acta Metall,1978;26:1293 [8]Zhang Q Y,Zhuang H S.Handbook of Welding.Beijing: China Machine Presss,1998:38 (张启运,庄鸿寿.钎焊手册.北京:机械工业出版社, 1998: 38) [9]Pan W,Li R T,Chen J,Sun R F,Lian J.Mater Sci Eng, 2000;287:72 [10]Cui P.J Hefei Univ Technol,2002;25:365 (崔鹏.合肥工业大学学报, 2002;25:365) [11]Yang X M.Semicond Optoelect,2002;23:274 (杨雪梅.半导体光电,2002;23:274) [12]Murray J L,Bhansali K J.Bull Alloy Phase Diagram, 1983:4:178 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|