| Investigation Of Stability And Hydrogen Storage Properties Of LaNi5-XMx(M=Al, Mn) Alloys |
| ZHANG Ruijing; LŰ Manqi; CHEN Demin; YANG Ke |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
张瑞静; 吕曼祺; 陈德敏; 杨柯 . LaNi5-xMx(M=Al, Mn)合金的稳定性及储氢性能研究[J]. 金属学报, 2005, 41(4): 427-432 .
,
,
,
,
.
Investigation Of Stability And Hydrogen Storage Properties Of LaNi5-XMx(M=Al, Mn) Alloys[J]. Acta Metall Sin, 2005, 41(4): 427-432 .
[1]Kuijpers F A, Loopstra B O. J Phys Chem Sol, 1974; 35: 301 [2]Nakamura H, Nguyen-Manh D, Pettifor D G. J Alloys Compd, 1998; 281: 81 [3]Kisi E H, Wu E, Kemali M. J Alloys Compd, 2002; 330- 332: 202 [4]Wang X L, Suda S. Z Phys Chem, 1989; 164: 1235 [5]Dayan D, Mintz M H. J Less-Common Met, 1980; 73: 15 [6]Paul-Boncour V, Joubert J M, Latroche M, Percheron- Guegan A. J Alloys Compd, 2002; 330-332: 246 [7]Mendelsohn M H, Gruen D M, Dwight A E. Nature, 1977; 269: 45 [8]Takeshita T, Malik S K, Wallace W E. J Solid State Chem, 1978; 23: 271 [9]Mendelsohn M H, Gruen D M, Dwight A E. J Leas-Common Met, 1979; 63: 193 [10]Lartigue C, Percheron-Guegan A, Achard J G, Tasset F. J Less-Common Met, 1980; 75: 23 [11]Ide T, Sakai F, Yorozu M. Fusion Technol, 1988; 14: 769 [12]Xiao J M, Zhu F W. The Subject of Materials Energy. Shanghai: Shanghai Science & Technology Press, 1999: 256 (肖纪美,朱逢吾.材料能量学.上海:上海科技出版社,1999: 256) [13]Zhao S, Lin Q, Chen N, Ma L, Ye W. Ada Metall Sir, 1999;35:65 (赵爽,林勤,陈宁,马丽,叶文.金属学报,1999; 35:65) [14]Szajek A, Jurczyk M, Rajewski W. J Alloys Compd, 2000; 307: 290 [15]Westlake D G. J Less-Common Met, 1983; 91: 1 [16]Zhang R J, Lu M Q, Cao D L, Chen D M, Yang K. Rare Met, 2004; 28: 678 (张瑞静,吕曼祺,曹大力,陈德敏,杨柯.稀有金属,2004; 28:678) [17]Lartigue C, Percheron-Guegan A, Achard J G. J Less-Common Met, 1980; 75: 23 [18]Walters R T. J Less-Common Met, 1990; 157: 97 [19]Percheron-Guegan A, Latigue C, Achard J C, Germi P, Tasset F. J Less-Common Met, 1980; 74: 1 [20]Luder C E, Lynch F E, Magee C B. J Less-Common Met, 1977; 56: 19 [21]Switendick A C. Z Phys Chem, 1979; 117: 89 [22]Westlake D G. J Less-Common Met, 1980; 75: 177 [23]Westlake D G. J Less-Common Met, 1983; 90: 251 [24]Westlake D G. J Less-Common Met, 1983; 91: 275 [25]Lartigue C, Percheron-Guegan A, Achard J C. J Less Common Met, 1984; 101: 391 [26]Miedema A R. J Less-Common Met, 1975; 41: 283; 1976; 46: 67 [27]Gruen D M, Mendelsohn M. J Less-Common Met, 1977; 55: 149 [28]Percheron-Guegan A, Lartigue C, Achard J G. J Less-Common Met, 1985; 109: 287 [29]Gupta M. J Alloys Compd, 1999; 293-295: 190 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|